1

Topic: Eryone PLA with Minimaker : any successes?

I'm using Ntag hack with my Minimaker and I bought Eryone PLA. I can't get the filament to load properly without clogging the hotend. Anyone has successes with this PLA? What are the settings or the tricks?

2

Re: Eryone PLA with Minimaker : any successes?

Eryone PLA is garbage for me. I have never had it work on any of my machines.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Eryone PLA with Minimaker : any successes?

Ah man, I have a bunch of spools from them since they were available... Now I guess I know why!

carl_m1968 wrote:

Eryone PLA is garbage for me. I have never had it work on any of my machines.

4

Re: Eryone PLA with Minimaker : any successes?

Well, I had some issues with an older black xyz pla and wanted to try something different. Currently checking out Eryone spool and I am 50/50 on it. I printed several calibration blocks and came up with 215deg / 210deg. But when I tried to print something bigger the head clogged in a very messy way. And then the bowden tube came off from the feeder and more clogs. After replacing the feeder fitting (thanks to info on this site) I got the trusty xyz white pla and everything is back to normal. I will give the eryone black pla another try soon, but not to much success with it (it is really nicely wounded, but little that serves me).