1

Topic: CR10-S gaps in print/all layers

Printer:CR10-S
E3D head
Filament: Gizmo 1.75mm ABS/.04 nozzle
Temp: 228/80
I think this picture says it all!

Post's attachments

missing filament in print.jpg 3.45 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: CR10-S gaps in print/all layers

looks like the g code is programmed to print a raft.

Soliddoodle 4 stock w glass bed------Folger Tech Prusa 2020 upgraded to and titan /aero extruder mirror bed
FT5 with titan/ E3D Aero------MP mini select w glass bed
MP Utimate maker pro-W bondtech extruder
Marlin/Repetier Host/ Slic3r and Cura

3 (edited by carl_m1968 2019-11-13 12:34:21)

Re: CR10-S gaps in print/all layers

Now we have two post with responses on them as I already responded to his other post of the same. Could a mod please merge these?

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.