My XYZ prints fine until I get into the higher mm layers of the print in where it just wont print evenly and i end up with a messy top half of a print. Maybe someone has had this experience with this. Maybe the Gentry X rails?!

Post's attachments

18mm ring EZABL mount.jpg
18mm ring EZABL mount.jpg 3.12 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Higher layers in print fall apart

try lower nozzle temperature and add layer cooling fan mod. What is the printer model anywayv