I wanted to create a metallic material ended up with this

http://soliforum.com/i/?LOtVCLY.jpg
http://soliforum.com/i/?ojhVMw1.jpg

2

Re: Wood filament

MohG wrote:

I wanted to create a metallic material ended up with this

http://soliforum.com/i/?LOtVCLY.jpg
http://soliforum.com/i/?ojhVMw1.jpg


You should checkout Protopasta. They make filaments that have metal powders in them and can even be polished like the real metal once printed. They have copper, steel, I believe bronze is even available.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Wood filament

wanted to make sth metallic ended up with a wood-like material as you see in the pics...ABS pellets with gold metallic paint