1

Topic: (S4) Support material help (pics)

Greetings,
I need some help with support materials on my S4. I recently upgraded to the E3D Lite6 and havent had much luck with my support materials, and been cuting pieces like cray to avoid using support materials. But sometimes, I just have to and doesnt turn out too well.
I do have a extrusion calibrated and bed leveled best I can. But this is what I get

http://i.imgur.com/6sXWJR4.jpg

http://i.imgur.com/qV9HHwQ.jpg

http://i.imgur.com/SETXb6g.jpg

Here are my settings

http://i.imgur.com/swFKapE.jpg

Any help would be much appriciated

2

Re: (S4) Support material help (pics)

What speed are you running?

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: (S4) Support material help (pics)

Most importantly, get us a screenshot of your extrusion width settings.  It's in the advanced tab, looks as though that may be way off.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

4

Re: (S4) Support material help (pics)

yes, speed and extrusion widths...

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

5

Re: (S4) Support material help (pics)

Hello,
Here is my Speed setting tab and my Extrusion widths

http://i.imgur.com/HvlmTtM.png

http://i.imgur.com/JXrzCdG.png

Thanks again for all the help

6

Re: (S4) Support material help (pics)

Your infill is way too fast and probably beyond your printers capabilities. I would lower it to 35 max.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

7

Re: (S4) Support material help (pics)

An extrusion width of .2 is far too low, try .36
As for speeds, your settings seem to be all over the place.  That machine in basically stock form should have no problems with 60mm/second depending on acceleration rates set in the firmware. 
In stock form acceleration rates are slow enough to allow 60mm/second.  With the proper mods 120mm/second is very doable.  Set all your speeds at 60 except bridging (slow down about 75%)
Infill can be slowed slightly (maybe 50).

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

8

Re: (S4) Support material help (pics)

Here are my settings for my SD4.  This particular preset is a slower one I use for highly accurate prints; it may give you something to compare with.

Speed settings:

https://www.dropbox.com/s/tyhzbwaeza1x9zh/Speed%20settings.PNG?dl=1


Advanced settings: