Topic: TPE pellets where???

Why is it so f****** hard to find anyone selling flexible pellets in europe??
I haven't found a single one yet.

IF you find any in US the cost of shipping is 10times more than the actual pellets cost.

Do ANYONE have any info about the TPE pellets Revolve3D sold and where to get them?
I mailed them the question but did not answer me.

Would a SHORE A 55 work?
I know the Ninjaflex is A 85. And the Alphagary 3019 i tried i think was A 40/45 (way to to soft),
it worked when printing VERY slow (5mm/s) but it SMELLED like ass when extruding and printing.

2

Re: TPE pellets where???

hi all
i ve  found this one in europe
http://pix.slic.it/p/42o
http://pix.slic.it/p/42p
not tpe  but tpu
the flexibility is very high
is very dificult to extrud a flexible filament , start with pla pellet like this

look the product during  mini makerfaire  Torino (italy)  06.06.2015
https://www.youtube.com/watch?v=__LoLItqIrY
regards
fredaxe

3

Re: TPE pellets where???

Where? It's just pictures, no adress or so.

Well i want something like ninjaflex. The revolve3d pellets were just like ninja.
I have more than a year expericence in extruding PLA, ABS and some flex.
Revolve3d's flexible pellets were not difficult to extrude, somewhere between ABS and PLA.

(TPE will stretch but not compress the same amount.TPU both compress and expand the same.)
if i have understood correctly.

fredaxe wrote:

hi all
i ve  found this one in europe
http://pix.slic.it/p/42o
http://pix.slic.it/p/42p
not tpe  but tpu
the flexibility is very high
is very dificult to extrud a flexible filament , start with pla pellet like this

look the product during  mini makerfaire  Torino (italy)  06.06.2015
https://www.youtube.com/watch?v=__LoLItqIrY
regards
fredaxe