Re: Melt filters now available
Rusty bin? I think you're talking about Octave black filament*
*and frankly any other cheap filament producer's black filament.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → Melt filters now available
Rusty bin? I think you're talking about Octave black filament*
*and frankly any other cheap filament producer's black filament.
I think the filastruder is flat out awesome. From what it was in the beginning to now, its great. I finally passed the fight with extruding PLA at the correct diameter and my prints turn out much better than when using mgchemical filament! Good job Tim and Ian. The filawinder, hasn't let me down since I replaced the hall sensor. (had a broken leg and intermittent sensing) After that its been winding away!