<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Even coloring?]]></title>
		<link>https://www.soliforum.com/topic/9810/even-coloring/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/9810/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Even coloring?.]]></description>
		<lastBuildDate>Mon, 09 Feb 2015 07:26:07 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Even coloring?]]></title>
			<link>https://www.soliforum.com/post/84215/#p84215</link>
			<description><![CDATA[<p>I&#039;ve been reading through the forums and have seen people say that the grinder doesn&#039;t really work very well. If you know of one that does work, it&#039;d be great if you could let me know the brand/model.<br />I saw something about liquid colorants, do those work well? Where can I order those and the powder colorants.</p>]]></description>
			<author><![CDATA[null@example.com (sue121507)]]></author>
			<pubDate>Mon, 09 Feb 2015 07:26:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/84215/#p84215</guid>
		</item>
		<item>
			<title><![CDATA[Re: Even coloring?]]></title>
			<link>https://www.soliforum.com/post/84166/#p84166</link>
			<description><![CDATA[<p>This has been covered several times. The approaches are:</p><p>- assemble properly<br />- use quality colorant designed for the material you&#039;re extruding<br />- use a burr grinder to reduce the colorant size<br />- mix at high concentration (4:1), extrude, pelletize, mix with virgin material at closer to 10:1, extrude</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 08 Feb 2015 23:26:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/84166/#p84166</guid>
		</item>
		<item>
			<title><![CDATA[Even coloring?]]></title>
			<link>https://www.soliforum.com/post/84159/#p84159</link>
			<description><![CDATA[<p>How do you get the most even coloring? I have the pellets, so I want to be able to use those, I&#039;ve seen people say that the color isn&#039;t always that even though with the pellets, so what&#039;s the best way to make it even? Also where do you get the powdered colors from?</p>]]></description>
			<author><![CDATA[null@example.com (sue121507)]]></author>
			<pubDate>Sun, 08 Feb 2015 23:01:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/84159/#p84159</guid>
		</item>
	</channel>
</rss>