<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Bronzefill or Woodfill with the Davinci ?]]></title>
		<link>https://www.soliforum.com/topic/9643/bronzefill-or-woodfill-with-the-davinci/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/9643/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Bronzefill or Woodfill with the Davinci ?.]]></description>
		<lastBuildDate>Fri, 27 May 2016 07:37:42 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/123486/#p123486</link>
			<description><![CDATA[<p>Etxremely difficult time with this stuff today.&nbsp; Turns out I have Esun brand.</p><p>I think 4mm retraction was my issue, as the heatbreak of the v6 ended up getting clogged half way through the print.</p><p>You really gotta keep this stuff flowing fast!</p>]]></description>
			<author><![CDATA[null@example.com (Telemachus)]]></author>
			<pubDate>Fri, 27 May 2016 07:37:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/123486/#p123486</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/123433/#p123433</link>
			<description><![CDATA[<p>You should be ok with those settings.<br />I use Fillamentum Timberfill these days, seems a bit easier to print.<br />I have retraction set at 4mm as you get a lot of stringing with it, I would think Woodfill will be similar.</p>]]></description>
			<author><![CDATA[null@example.com (scobo)]]></author>
			<pubDate>Thu, 26 May 2016 07:13:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/123433/#p123433</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/123406/#p123406</link>
			<description><![CDATA[<p>I got some woodfill last night, colorfabb brand.</p><p>Print it with mostly PLA settings?&nbsp; Is 35mm/sec speed ok?</p><p>From what I read, you can&#039;t let it sit in the extruder long.</p>]]></description>
			<author><![CDATA[null@example.com (Telemachus)]]></author>
			<pubDate>Wed, 25 May 2016 21:17:52 +0000</pubDate>
			<guid>https://www.soliforum.com/post/123406/#p123406</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101920/#p101920</link>
			<description><![CDATA[<p>Interesting info! </p><p>Thanks</p>]]></description>
			<author><![CDATA[null@example.com (mrtjahzi)]]></author>
			<pubDate>Fri, 24 Jul 2015 09:35:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101920/#p101920</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101325/#p101325</link>
			<description><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>the fan always turns with the same rpm? for example if I active the bridging option 100% fan I would have a difference?</p></blockquote></div><p>There is no control of that fan, the Repetier firmware does not have access to the pins that operate that fan. Just stop trying to control it and don&#039;t worry about what it does. It will not hurt your print for it to run all the time.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Thu, 16 Jul 2015 17:30:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101325/#p101325</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101313/#p101313</link>
			<description><![CDATA[<p>the fan always turns with the same rpm? for example if I active the bridging option 100% fan I would have a difference?</p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Thu, 16 Jul 2015 16:41:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101313/#p101313</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101261/#p101261</link>
			<description><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><div class="quotebox"><cite>efes wrote:</cite><blockquote><p>I do not feel that the FAN on the extruder running!<br />but hey I find the solution by removing the fan plug <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p></blockquote></div><p>The fan on the Da Vinci unless you have modified the extruder to something else is not a layer fan and should always be on. It&#039;s purpose is to cool the actual extruder and feed tube. The printer is mad for ABS and the fan/extruder in stock form will have no impact on printing ABS. Do not turn it off or you will damage the extruder and motor.</p></blockquote></div><br /><p>oups ! I reconnect the plug!<br />So if I understand with DaVinci 1.0 and firmware repetier fan must always turned even with ABS?</p></blockquote></div><p>That is correct. I think your confusion is with what people say about PLA. With PLA they recommend you turn your layer fan off for the first one or two layers. This is for PLA only. For ABS you can but normally dont use a layer fan. The Da Vinci 1.0 in stock form unless modified like Scobo did or with a hotend remake can not print PLA and that is why it does not have s layer fan. </p><p>Again the stock fan is to cool the feed tube and extruder so heat soak does not make it hot enough to prematurely melt filament and cause grinding or jams.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 15 Jul 2015 22:31:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101261/#p101261</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101257/#p101257</link>
			<description><![CDATA[<p>ok..<br />another beer for CARL <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p><p><span class="postimg"><img src="http://www.macewans.fr/wp-content/uploads/2014/06/hoegaarden-verre-a-biere-500x500_2.png" alt="http://www.macewans.fr/wp-content/uploads/2014/06/hoegaarden-verre-a-biere-500x500_2.png" /></span></p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:47:52 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101257/#p101257</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101256/#p101256</link>
			<description><![CDATA[<p>As Carl says, it won&#039;t affect your prints anyway so there&#039;s no advantage in turning it off.<br />Although, I turn mine off in order to get the extruder up to temp quicker then turn it on as soon as it reaches the required temp.</p>]]></description>
			<author><![CDATA[null@example.com (scobo)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:45:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101256/#p101256</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101255/#p101255</link>
			<description><![CDATA[<div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><div class="quotebox"><cite>efes wrote:</cite><blockquote><p>I do not feel that the FAN on the extruder running!<br />but hey I find the solution by removing the fan plug <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p></blockquote></div><p>The fan on the Da Vinci unless you have modified the extruder to something else is not a layer fan and should always be on. It&#039;s purpose is to cool the actual extruder and feed tube. The printer is mad for ABS and the fan/extruder in stock form will have no impact on printing ABS. Do not turn it off or you will damage the extruder and motor.</p></blockquote></div><br /><p>oups ! I reconnect the plug!<br />So if I understand with DaVinci 1.0 and firmware repetier fan must always turned even with ABS?</p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:40:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101255/#p101255</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101254/#p101254</link>
			<description><![CDATA[<p>me FFF setting simplif3d ABS fan problem ?</p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:36:44 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101254/#p101254</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101253/#p101253</link>
			<description><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>I do not feel that the FAN on the extruder running!<br />but hey I find the solution by removing the fan plug <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p></blockquote></div><p>The fan on the Da Vinci unless you have modified the extruder to something else is not a layer fan and should always be on. It&#039;s purpose is to cool the actual extruder and feed tube. The printer is mad for ABS and the fan/extruder in stock form will have no impact on printing ABS. Do not turn it off or you will damage the extruder and motor.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:32:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101253/#p101253</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101252/#p101252</link>
			<description><![CDATA[<p>If you save your print as a factory file then upload it here, I could take a look at your Simplify3d settings. <br />There must be something turning the fan on at some point.</p>]]></description>
			<author><![CDATA[null@example.com (scobo)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:30:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101252/#p101252</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101251/#p101251</link>
			<description><![CDATA[<p>I do not feel that the FAN on the extruder running!<br />but hey I find the solution by removing the fan plug <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:27:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101251/#p101251</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bronzefill or Woodfill with the Davinci ?]]></title>
			<link>https://www.soliforum.com/post/101247/#p101247</link>
			<description><![CDATA[<p>Sorry, don&#039;t quite follow you.<br />Do you mean the fan comes on but you don&#039;t want it to ?</p>]]></description>
			<author><![CDATA[null@example.com (scobo)]]></author>
			<pubDate>Wed, 15 Jul 2015 21:06:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/101247/#p101247</guid>
		</item>
	</channel>