<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Apprentice extruder max temp?]]></title>
		<link>https://www.soliforum.com/topic/9597/apprentice-extruder-max-temp/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/9597/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Apprentice extruder max temp?.]]></description>
		<lastBuildDate>Fri, 30 Jan 2015 17:21:29 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Apprentice extruder max temp?]]></title>
			<link>https://www.soliforum.com/post/82405/#p82405</link>
			<description><![CDATA[<p>Thanks and nice work Solidoodle! That actually looks pretty professional!</p>]]></description>
			<author><![CDATA[null@example.com (jagowilson)]]></author>
			<pubDate>Fri, 30 Jan 2015 17:21:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82405/#p82405</guid>
		</item>
		<item>
			<title><![CDATA[Re: Apprentice extruder max temp?]]></title>
			<link>https://www.soliforum.com/post/82401/#p82401</link>
			<description><![CDATA[<p>Here are some quick pictures of the instructions. Just ask if something is unclear and you want a closer and better pic...<br /><a href="http://imgur.com/i9wcx2X,9M3cPjc,fVDLnwq,auiniN6,qkQ9PHO,ncK6gVb,nWypVKL,Pu2WVfa,iDkCO7z">http://imgur.com/i9wcx2X,9M3cPjc,fVDLnw … fa,iDkCO7z</a></p>]]></description>
			<author><![CDATA[null@example.com (Highender)]]></author>
			<pubDate>Fri, 30 Jan 2015 17:14:44 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82401/#p82401</guid>
		</item>
		<item>
			<title><![CDATA[Re: Apprentice extruder max temp?]]></title>
			<link>https://www.soliforum.com/post/82383/#p82383</link>
			<description><![CDATA[<p>We usually use 215, but anywhere from 200-220 should work. You may need to experiment a little and find what works best for you and the filament you are using. The firmware has a max temp of 230 so if either extruder reaches that all heaters will be shut off.</p>]]></description>
			<author><![CDATA[null@example.com (soliryan)]]></author>
			<pubDate>Fri, 30 Jan 2015 15:52:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82383/#p82383</guid>
		</item>
		<item>
			<title><![CDATA[Re: Apprentice extruder max temp?]]></title>
			<link>https://www.soliforum.com/post/82372/#p82372</link>
			<description><![CDATA[<p>The thermistor isn&#039;t at the nozzle so the temp readings aren&#039;t as accurate. The book instructions are correct.</p><p>Could you post some pictures of the instructions manual? Just curious. This is the first SD machine I know of to include one.</p>]]></description>
			<author><![CDATA[null@example.com (jagowilson)]]></author>
			<pubDate>Fri, 30 Jan 2015 15:15:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82372/#p82372</guid>
		</item>
		<item>
			<title><![CDATA[Apprentice extruder max temp?]]></title>
			<link>https://www.soliforum.com/post/82371/#p82371</link>
			<description><![CDATA[<p>In the instructions manual for the apprentice printer is says that the extruder can do 0-210 degrees C, But the ABS i got from Solidoodle has a recommended print temperature that is 230C + (or something, don&#039;t quite remember....) <br />Is it just a typo in the manual or should I not go over that temperature? As I have understood, most ABS filament needs a higher temperature than 210 to print. So when Solidoodle wrote that it could print ABS and PLA was they wrong?</p>]]></description>
			<author><![CDATA[null@example.com (Highender)]]></author>
			<pubDate>Fri, 30 Jan 2015 15:10:35 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82371/#p82371</guid>