<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — support material]]></title>
		<link>https://www.soliforum.com/topic/9324/support-material/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/9324/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in support material.]]></description>
		<lastBuildDate>Mon, 19 Jan 2015 02:51:10 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: support material]]></title>
			<link>https://www.soliforum.com/post/80069/#p80069</link>
			<description><![CDATA[<p>Also what shape do are you using for supports...Ive yet to use them but maybe somebody can chime in with pros and cons of some</p>]]></description>
			<author><![CDATA[null@example.com (OneMoreCast)]]></author>
			<pubDate>Mon, 19 Jan 2015 02:51:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/80069/#p80069</guid>
		</item>
		<item>
			<title><![CDATA[Re: support material]]></title>
			<link>https://www.soliforum.com/post/80050/#p80050</link>
			<description><![CDATA[<p>I set the offsets in repetier host in the x/y to somewhere between 0.3 and 0.8 mm and the z between 0.15 and 0.5mm. I assume you are referring to angle with 45 or 90, I actually usually set the overhang threshold to 60 degrees.</p>]]></description>
			<author><![CDATA[null@example.com (Devestat)]]></author>
			<pubDate>Mon, 19 Jan 2015 00:47:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/80050/#p80050</guid>
		</item>
		<item>
			<title><![CDATA[support material]]></title>
			<link>https://www.soliforum.com/post/80033/#p80033</link>
			<description><![CDATA[<p>what are you all running in your setting for support material settings to make it come off better ?? 90 or 45</p>]]></description>
			<author><![CDATA[null@example.com (cpsmicahel)]]></author>