<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Filament "clicking" on larger print areas]]></title>
		<link>https://www.soliforum.com/topic/926/filament-clicking-on-larger-print-areas/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/926/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filament "clicking" on larger print areas.]]></description>
		<lastBuildDate>Fri, 04 Jan 2013 17:33:43 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filament "clicking" on larger print areas]]></title>
			<link>https://www.soliforum.com/post/8505/#p8505</link>
			<description><![CDATA[<p>Easy enough to clean out the extruder with a soft brush and a vacuum cleaner</p>]]></description>
			<author><![CDATA[null@example.com (jon_bondy)]]></author>
			<pubDate>Fri, 04 Jan 2013 17:33:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/8505/#p8505</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament "clicking" on larger print areas]]></title>
			<link>https://www.soliforum.com/post/8490/#p8490</link>
			<description><![CDATA[<p>Over time the amount of filament dust from these skipped clicks add up and smooth out the filament drive wheel.</p><p>not really a worry, (try a slower speed or hotter temp to fix)</p><p>but if this happens a lot it can get progressively worse as the crap builds up in the extruder</p>]]></description>
			<author><![CDATA[null@example.com (danny)]]></author>
			<pubDate>Fri, 04 Jan 2013 14:55:35 +0000</pubDate>
			<guid>https://www.soliforum.com/post/8490/#p8490</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament "clicking" on larger print areas]]></title>
			<link>https://www.soliforum.com/post/8378/#p8378</link>
			<description><![CDATA[<p>What color is the filament, this seems like the problem that some people were having with a batch of black filament from solidoodle.&nbsp; I remember this being talked about and it had something to do with increasing the extruder temp and pressure on the tensioner.&nbsp; I tried to find the thread but I came up empty.&nbsp; I could have sworn it was a post from solidoodle support.&nbsp; Maybe someone else remembers where the thread was.</p>]]></description>
			<author><![CDATA[null@example.com (cmetzel)]]></author>
			<pubDate>Thu, 03 Jan 2013 14:57:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/8378/#p8378</guid>
		</item>
		<item>
			<title><![CDATA[Filament "clicking" on larger print areas]]></title>
			<link>https://www.soliforum.com/post/8373/#p8373</link>
			<description><![CDATA[<p>Sometimes when I am on a large print section, or just feeding 25+mm of filament through the heated extruder, the filament skips or &quot;clicks&quot;.&nbsp; It is like too much filament is trying to get fed at one time, so the gear that feeds the filament skips a bit.</p><p>Is this something to be concerned about, or is that just normal sometimes?</p><p>The sound drives me crazy because I am not sure if it is okay or not.</p><p>I&#039;ve tried tightening and/or loosening the adjustment screw that puts tension onto the extruder gear, but that has not helped.</p><p>Should I make adjustments elsewhere?</p><p>Thanks!</p>]]></description>