		<title><![CDATA[SoliForum - 3D Printing Community — 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
		<link>https://www.soliforum.com/topic/8774/285mm-filastruder-users-what-nozzle-size-has-worked-the-best/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/8774/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in 2.85mm Filastruder Users- What nozzle size has worked the best?.]]></description>
		<lastBuildDate>Mon, 28 Nov 2016 16:16:40 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/128435/#p128435</link>
			<description><![CDATA[<p>Hi All,</p><p>I just bought my filastruder and have a Ultimaker, so I would like to make 3.0mm filament with ABS MG-94, do you have any recomendation for the first test?</p><p>Cheers</p>]]></description>
			<author><![CDATA[null@example.com (JoaoGripp)]]></author>
			<pubDate>Mon, 28 Nov 2016 16:16:40 +0000</pubDate>
			<guid>https://www.soliforum.com/post/128435/#p128435</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75823/#p75823</link>
			<description><![CDATA[<p>I&#039;m currently extruding black ABS and am getting a little over 3 in / min.</p>]]></description>
			<author><![CDATA[null@example.com (bbriggsgeek)]]></author>
			<pubDate>Fri, 19 Dec 2014 12:25:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75823/#p75823</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75615/#p75615</link>
			<description><![CDATA[<p>What kind of speeds are you seeing? What material?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Wed, 17 Dec 2014 22:03:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75615/#p75615</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75614/#p75614</link>
			<description><![CDATA[<p>I have mine mounted vertically which tends to make the filament thinner.&nbsp; I have gradually drilled mine out to 3.2mm.&nbsp; I try to keep my filament between 2.9 and 3.0 mm.</p>]]></description>
			<author><![CDATA[null@example.com (bbriggsgeek)]]></author>
			<pubDate>Wed, 17 Dec 2014 21:48:44 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75614/#p75614</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75607/#p75607</link>
			<description><![CDATA[<div class="quotebox"><cite>bbriggsgeek wrote:</cite><blockquote><p>I drilled mine out to give me faster extrusion.&nbsp; Temperature also affects diameter.</p></blockquote></div><p>What size drill but did you use?</p>]]></description>
			<author><![CDATA[null@example.com (Ggalisky)]]></author>
			<pubDate>Wed, 17 Dec 2014 20:12:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75607/#p75607</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75596/#p75596</link>
			<description><![CDATA[<p>I drilled mine out to give me faster extrusion.&nbsp; Temperature also affects diameter.</p>]]></description>
			<author><![CDATA[null@example.com (bbriggsgeek)]]></author>
			<pubDate>Wed, 17 Dec 2014 17:26:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75596/#p75596</guid>
		</item>
		<item>
			<title><![CDATA[Re: 2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75517/#p75517</link>
			<description><![CDATA[<p>Standard nozzle can do 3mm or 2.85mm depending on extrusion temperature and height from the floor/bottom of the loop. It is drilled to 2.77mm.</p><p>Extruding: Not much difference. Filawinding: You&#039;ll need to move the PTFE holder further away so the servo doesn&#039;t have to flex the filament as much to move it back and forth on the spool.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Wed, 17 Dec 2014 01:42:23 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75517/#p75517</guid>
		</item>
		<item>
			<title><![CDATA[2.85mm Filastruder Users- What nozzle size has worked the best?]]></title>
			<link>https://www.soliforum.com/post/75511/#p75511</link>
			<description><![CDATA[<p>Does the standard 3mm Filastruder nozzle produce 2.85mm, or has anyone drilled out their nozzle and found better results? I am starting to experiment with 3mm so thanks!</p><p>Also, what are the major differences in extruding and filawinding 2.85mm?</p>]]></description>
			<author><![CDATA[null@example.com (Ggalisky)]]></author>
			<pubDate>Wed, 17 Dec 2014 01:09:23 +0000</pubDate>
			<guid>https://www.soliforum.com/post/75511/#p75511</guid>
		</item>