<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — XYZWare fails to export]]></title>
		<link>https://www.soliforum.com/topic/8161/xyzware-fails-to-export/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/8161/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in XYZWare fails to export.]]></description>
		<lastBuildDate>Wed, 29 Oct 2014 01:50:01 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: XYZWare fails to export]]></title>
			<link>https://www.soliforum.com/post/70052/#p70052</link>
			<description><![CDATA[<p>Good Call.<br />I just discovered that site here on this forum a few minutes ago.<br />I was able to get a good export from XYZware after using the STL repair service.<br />Thanks for the quick (and useful) answer!<br />-print3d</p>]]></description>
			<author><![CDATA[null@example.com (print3d)]]></author>
			<pubDate>Wed, 29 Oct 2014 01:50:01 +0000</pubDate>
			<guid>https://www.soliforum.com/post/70052/#p70052</guid>
		</item>
		<item>
			<title><![CDATA[Re: XYZWare fails to export]]></title>
			<link>https://www.soliforum.com/post/70051/#p70051</link>
			<description><![CDATA[<p>Run your STL thru modelrepair.azurewebsites.net but the larger issue could be that Slic3r isn&#039;t that great for complex stuff and xyzware uses slic3r.</p>]]></description>
			<author><![CDATA[null@example.com (skywiselh)]]></author>
			<pubDate>Wed, 29 Oct 2014 01:43:02 +0000</pubDate>
			<guid>https://www.soliforum.com/post/70051/#p70051</guid>
		</item>
		<item>
			<title><![CDATA[XYZWare fails to export]]></title>
			<link>https://www.soliforum.com/post/70049/#p70049</link>
			<description><![CDATA[<p>Hi all.</p><p>I&#039;m trying to print a battery holder that I found on thingiverse (456900)<br />I used scad to generate an STL (triple-D cell configuration) and all looks good when I import into XYZware.</p><p>When I export to .3w the serpentine springs are missing in the rendered model...WTH?!?!<br />I&#039;ve tried many quality options, with and without rafting/supports, without success.</p><p>I&#039;ve tried the latest xyzware (1.32, IIRC) and also 1.30.<br />1.30 took a LONG time to slice but eventually came up with the same result.</p><p>Any suggestions to try to make XYZware behave?</p><p>-print3d</p>]]></description>
			<author><![CDATA[null@example.com (print3d)]]></author>
			<pubDate>Wed, 29 Oct 2014 01:13:22 +0000</pubDate>