<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Print not completing.]]></title>
		<link>https://www.soliforum.com/topic/8042/print-not-completing/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/8042/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Print not completing..]]></description>
		<lastBuildDate>Mon, 20 Oct 2014 00:31:16 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69138/#p69138</link>
			<description><![CDATA[<p>check first time&nbsp; prints in netfab before slicing then page through Gcode b4 printing I have found lots of odd things either added or removed that way instead of descovering it while trying to print and seeing strange results lol</p>]]></description>
			<author><![CDATA[null@example.com (n2ri)]]></author>
			<pubDate>Mon, 20 Oct 2014 00:31:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69138/#p69138</guid>
		</item>
		<item>
			<title><![CDATA[Re: Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69115/#p69115</link>
			<description><![CDATA[<p>I have been just tried to do one to many pint in the center of the bed without freshening up the surface. </p><p>Well the print completed but a rough finish guess i need to figure out the cura settings seems like slic3r has a lot more control . but it just will not complete the slicing on this file. I tried the older software still no joy. <br />the happy Halloween headless dog. Oh well only plastic.<br />it is demonstrator to show the infill yea that&#039;s it!!! I stopped the print on purpose in the same spot twice !!<br />If this was easy everyone would be doing it. Easy stuff 5 year old can do this with 10&nbsp; years experience . but home level 3 d printers have only been available for 3 years!! anyway life goes on. </p><p>Tin</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Sun, 19 Oct 2014 22:53:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69115/#p69115</guid>
		</item>
		<item>
			<title><![CDATA[Re: Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69085/#p69085</link>
			<description><![CDATA[<p>Use glass and aquanet man. No need to fight adhesion trouble. Haven&#039;t had a print pop off since. Rip up the kapton too so you can get the glass off easily without knocking the bed out of level.</p>]]></description>
			<author><![CDATA[null@example.com (jagowilson)]]></author>
			<pubDate>Sun, 19 Oct 2014 21:27:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69085/#p69085</guid>
		</item>
		<item>
			<title><![CDATA[Re: Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69084/#p69084</link>
			<description><![CDATA[<p>well did as you said and it shows the poodle without a head. Looks like slicer did not complete the task. tried reslicing in cura looks better now trying to print been a bad day for printing one failure after another. <br />Had a print pop off the bed anther&nbsp; the print shiftedon another one probably my fault. .......</p><p>Thanks again <br />Tin</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Sun, 19 Oct 2014 20:56:17 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69084/#p69084</guid>
		</item>
		<item>
			<title><![CDATA[Re: Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69077/#p69077</link>
			<description><![CDATA[<p>On the Gcode tab in RH , click on &quot;show complete code&quot; and see if it shows the complete object.</p>]]></description>
			<author><![CDATA[null@example.com (satman49)]]></author>
			<pubDate>Sun, 19 Oct 2014 18:48:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69077/#p69077</guid>
		</item>
		<item>
			<title><![CDATA[Print not completing.]]></title>
			<link>https://www.soliforum.com/post/69046/#p69046</link>
			<description><![CDATA[<p>I have been at his about 10 weeks or so. Have done a lot of reading and some experimenting I have loaded the newer versions of RH and Slic3r&nbsp; Possibly the cause of my problem(s). I have had pretty good results so far and made a fair amount of good prints as well as some ugly ones. I have figured out the source of some problems <br />1) Rh has seemed reluctant to connect,&nbsp; last night no problem.<br />2) I fixed the isue of parking after the print. <br />the real and current question a&nbsp; I attempted to print a solidoodle poodle and it comes out headless. a second attempt did the same thing . <br />I have had prints quit before but not repeatedly in the same place in the print. <br />I checked the printer settings in rh and slicer and the print envelope setting look right. <br />The dog is only about 80mm high and the print stops at 60mm. <br />I am using a SD4 so plenty of room for this print. <br />Ideas?<br />Tin</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Sun, 19 Oct 2014 12:25:52 +0000</pubDate>
			<guid>https://www.soliforum.com/post/69046/#p69046</guid>