<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Where can I buy a filastruder?]]></title>
		<link>https://www.soliforum.com/topic/7976/where-can-i-buy-a-filastruder/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/7976/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Where can I buy a filastruder?.]]></description>
		<lastBuildDate>Mon, 13 Oct 2014 00:04:04 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Where can I buy a filastruder?]]></title>
			<link>https://www.soliforum.com/post/68477/#p68477</link>
			<description><![CDATA[<p>What Ian said, though GGalisky here on the forum can granulate for you.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 13 Oct 2014 00:04:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/68477/#p68477</guid>
		</item>
		<item>
			<title><![CDATA[Re: Where can I buy a filastruder?]]></title>
			<link>https://www.soliforum.com/post/68467/#p68467</link>
			<description><![CDATA[<p><a href="http://www.filastruder.com">www.filastruder.com</a></p><p>Recycling is hard however,&nbsp; expect to spend $400 minimum for a shredder.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Sun, 12 Oct 2014 22:05:59 +0000</pubDate>
			<guid>https://www.soliforum.com/post/68467/#p68467</guid>
		</item>
		<item>
			<title><![CDATA[Where can I buy a filastruder?]]></title>
			<link>https://www.soliforum.com/post/68466/#p68466</link>
			<description><![CDATA[<p>I&#039;d like to recycle and make my own filament. If I can&#039;t buy one are there plans to make them?</p>]]></description>
			<author><![CDATA[null@example.com (shields1.as)]]></author>
			<pubDate>Sun, 12 Oct 2014 22:02:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/68466/#p68466</guid>