		<title><![CDATA[SoliForum - 3D Printing Community — How do you wind filament on the spool ?]]></title>
		<link>https://www.soliforum.com/topic/7543/how-do-you-wind-filament-on-the-spool/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/7543/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in How do you wind filament on the spool ?.]]></description>
		<lastBuildDate>Sun, 07 Sep 2014 12:24:09 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65681/#p65681</link>
			<description><![CDATA[<p>80C? You might need longer, depending on how much moisture it had to begin with.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 07 Sep 2014 12:24:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65681/#p65681</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65679/#p65679</link>
			<description><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>Just like normal stuff. Did you dry yours? How?</p></blockquote></div><p>Did indeed, in the oven for about 2 hours at 80.<br />I suppose some experimentation is in order.</p>]]></description>
			<author><![CDATA[null@example.com (Serin)]]></author>
			<pubDate>Sun, 07 Sep 2014 12:15:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65679/#p65679</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65678/#p65678</link>
			<description><![CDATA[<p>Just like normal stuff. Did you dry yours? How?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 07 Sep 2014 12:03:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65678/#p65678</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65674/#p65674</link>
			<description><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>This is definitely wrong, I&#039;ve drill spooled with PLA and many others have used the FilaWinder with PLA.</p></blockquote></div><p>Curious, how flexible has your PLA been? The stuff I&#039;ve been putting out has been.. Quite fragile.<br />Is it a temp thing or just an artefact of the 4043D polymer?</p>]]></description>
			<author><![CDATA[null@example.com (Serin)]]></author>
			<pubDate>Sun, 07 Sep 2014 11:34:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65674/#p65674</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65671/#p65671</link>
			<description><![CDATA[<p>This is definitely wrong, I&#039;ve drill spooled with PLA and many others have used the FilaWinder with PLA.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 07 Sep 2014 11:04:21 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65671/#p65671</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65660/#p65660</link>
			<description><![CDATA[<p>Lesson of the day.<br />DOES NOT WORK WITH PLA.<br />Filawinder also no help. PLA is too hard and extruded with a twist that you absolutely have no choice but to twist with it, or else.<br />I got like 4LB of 1.75mm on the floor, thought i would get lucky <img src="https://www.soliforum.com/img/smilies/sad.png" width="15" height="15" alt="sad" /></p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Sun, 07 Sep 2014 07:27:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65660/#p65660</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65093/#p65093</link>
			<description><![CDATA[<p>I tried and failed at first. Went too fast and applied too much pressure on the string, thus not allowing it to twist while wrapping around the spool.<br />Slowed down and let the string more loose resolved the problem.</p><p>I knew people did it with drills but what i experienced told me &quot;its not gonna work&quot; and it make me spend more money.<br />OH well, too many toys is not too many women. I&#039;ll live <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 01 Sep 2014 23:12:40 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65093/#p65093</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65089/#p65089</link>
			<description><![CDATA[<p>I promise what I do in the video works fine. I&#039;ve done it for 120kg of filament so far. It doesn&#039;t have to be perfectly even, I&#039;ve never had a spool tangle while feeding the printer.</p><p>Why bother asking if you&#039;re not going to trust the advice of someone that has done it (a lot)?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 01 Sep 2014 22:52:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65089/#p65089</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65088/#p65088</link>
			<description><![CDATA[<p>In your example its not coiled even around its self. I cant take a spool and rotate it in one direction, filament will loop around its self after few turns.<br />Plus video showed few feet. I have few hundred feet to deal with.</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 01 Sep 2014 22:24:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65088/#p65088</guid>
		</item>
		<item>
			<title><![CDATA[Re: How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65086/#p65086</link>
			<description><![CDATA[<p>You don&#039;t need to rotate, you can stand still. I can wind 1kg in about 2 minutes. Here&#039;s a quick vid showing it:</p><p><a href="https://www.youtube.com/watch?feature=player_detailpage&amp;v=Pv2n5_xi56w#t=22">https://www.youtube.com/watch?feature=p … xi56w#t=22</a></p><p>I can take another video if you really need it, but it&#039;s pretty simple. Attach the spool to the drill, pull the trigger. You can get a cheap drill from Harbor Freight.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 01 Sep 2014 22:17:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65086/#p65086</guid>
		</item>
		<item>
			<title><![CDATA[How do you wind filament on the spool ?]]></title>
			<link>https://www.soliforum.com/post/65084/#p65084</link>
			<description><![CDATA[<p>Yep. How do you do it ?<br />The way i do it is to stand in the lopp middle of the piled up filament and hold/guide filament while twisting the spool.<br />At the same time i turn around so that filament wont loop around its self and bend or crack/brake.<br />This gets my wrist tired and make me dizzy for spinning around.</p><p>Is there a better way to do it without filawinder ?<br />I thought of cordless drill (that i dont have) but it will just make me spin faster.</p><p>I also tried going up the ladder but result is the same. Filament would loop around it self and tangle allover.</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 01 Sep 2014 22:05:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/65084/#p65084</guid>