<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Bad filament surface at higher temps]]></title>
		<link>https://www.soliforum.com/topic/7338/bad-filament-surface-at-higher-temps/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/7338/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Bad filament surface at higher temps.]]></description>
		<lastBuildDate>Sat, 16 Aug 2014 20:45:49 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Bad filament surface at higher temps]]></title>
			<link>https://www.soliforum.com/post/63523/#p63523</link>
			<description><![CDATA[<p>Hmm. It would be good to know, not only for expected extrusion properties but also for safety!</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 16 Aug 2014 20:45:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/63523/#p63523</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bad filament surface at higher temps]]></title>
			<link>https://www.soliforum.com/post/63522/#p63522</link>
			<description><![CDATA[<p>Ah good to know.<br />I dont know what kind of plastic I have</p>]]></description>
			<author><![CDATA[null@example.com (Sungod3000)]]></author>
			<pubDate>Sat, 16 Aug 2014 20:42:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/63522/#p63522</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bad filament surface at higher temps]]></title>
			<link>https://www.soliforum.com/post/63467/#p63467</link>
			<description><![CDATA[<p>This is pretty common with all ABS, though MG94 doesn&#039;t seem to do it until 200C or so. I am not certain if it is from moisture or melt fracture. Have you tried drying the pellets? What resin ID?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 16 Aug 2014 03:35:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/63467/#p63467</guid>
		</item>
		<item>
			<title><![CDATA[Bad filament surface at higher temps]]></title>
			<link>https://www.soliforum.com/post/63443/#p63443</link>
			<description><![CDATA[<p>Hey,</p><p>I have the issue that the surface of my ABS I bought from and injection molding company gets really rough when I extrude it over 175C. Its not really a problem it just looks weird. </p><p>I assume its an issue with that particular type of plastic, but I wanted to ask if anyone else has seen a similar thing with their extrusion.</p>]]></description>