<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Is there a better feeder screw ?]]></title>
		<link>https://www.soliforum.com/topic/7267/is-there-a-better-feeder-screw/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/7267/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Is there a better feeder screw ?.]]></description>
		<lastBuildDate>Mon, 11 Aug 2014 06:34:49 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62886/#p62886</link>
			<description><![CDATA[<p>Using an oven is too expensive. Cheap filament becomes not so cheap but &quot;i made it my self&quot; filament.<br />Air drying would be quicker and cheaper then using an oven for 2 hrs.<br />His drier container needs to have a cone shape on one side to make it easier to unload.</p><p>When i get rich, ill buy his setup <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> Its freaking awesome. Its like a mini factory that has it all.</p><p>Now my biggest question is: Where do i find 18-24 page rated <strong>micro cut</strong> paper/cd/dvd shredder for cheap, so i can use it to shred plastic such as milk bottles and other stuff as well as scraps from printing.</p><p>I attempted to do just that with my 12 page rated shredder and it was OK but not perfect. I had to run pieces thru couple of times because some were not broken apart but results were very impressive.<br /><a href="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5952&amp;preview">http://www.soliforum.com/misc.php?actio … mp;preview</a><br /><a href="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5953&amp;preview">http://www.soliforum.com/misc.php?actio … mp;preview</a></p><p>By the way, does anybody know how to post an image while forum doesnt provide direct link to image uploaded ?</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 11 Aug 2014 06:34:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62886/#p62886</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62884/#p62884</link>
			<description><![CDATA[<p>Hugh Lyman has an cool filament dryer in one of his videos, but I don&#039;t think he ever posted the files.&nbsp; It wouldn&#039;t be hard to recreate.</p><p><div class="fancy_video_tag_player"><iframe class="youtube-player" type="text/html" width="640" height="385" src="http://www.youtube.com/embed/o4F3e6K5Hxk" frameborder="0"></iframe></div></p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Mon, 11 Aug 2014 06:23:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62884/#p62884</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62878/#p62878</link>
			<description><![CDATA[<p>Darn it, another thing to buy <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /><br />Hopper can probably be eazy to design and print, but screen and hair dryer with variable speed (low) will need to be searched for at local thrift store.</p><p>But thats very very very cool !</p><p>Thanks !</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 11 Aug 2014 04:17:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62878/#p62878</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62876/#p62876</link>
			<description><![CDATA[<p>A hopper with mesh screens on the sides that blow hot, dry air up and through the hopper. </p><p><span class="postimg"><img src="http://www.qualityhindustan.com/hopper1.jpg" alt="http://www.qualityhindustan.com/hopper1.jpg" /></span></p><p>They have to do this for three reasons:</p><p>1.) They cannot tolerate any variation in their material properties. A typical industrial hopper would hold 6-12 hours of material, and industrial machines are even more sensitive than DIY machines since they process so much faster.<br />2.) Factories are typically not HVAC&#039;ed, and often damp/humid.<br />3.) They do not store the material sealed - it arrives in big cardboard boxes, called gaylords... or sometimes train cars. Thus they must dry it at some point, so best to dry it right before extrusion.</p><p>For DIY stuff, it seems drying it well before use, and only adding a few hours at a time of material (so material isn&#039;t sitting in the hopper all day) works well. Wouldn&#039;t hurt to use a lid. I&#039;ve only run PLA for 15-20 hours total, others here are probably far more experienced. I prefer ABS because much of what I print has to withstand high temperatures.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 11 Aug 2014 04:03:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62876/#p62876</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62875/#p62875</link>
			<description><![CDATA[<p>How do &quot;pros&quot; dry it in the hopper, what do you mean by that ? Removable hopper with a lid or something ?<br />Thanks !</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 11 Aug 2014 03:34:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62875/#p62875</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62874/#p62874</link>
			<description><![CDATA[<p><a href="http://www.natureworksllc.com/~/media/Technical_Resources/Processing_Guides/Fibers/ProcessingGuides_Meltblown_pdf.pdf">http://www.natureworksllc.com/~/media/T … wn_pdf.pdf</a></p><p>90C for 2-4 hours is appropriate. I would probably aim for 80C and closer to 4 hours to avoid melting the pellets, since Tg is around 70C.</p><p>Sealed and silica pack does not mean its dry. Not at all. The pros dry it inline, while its in the hopper - that&#039;s how important it is for there to be no moisture.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Mon, 11 Aug 2014 03:26:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62874/#p62874</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62873/#p62873</link>
			<description><![CDATA[<p>I had it dry to begin with, it came sealed and with silica pack inside. It worked fine untill it absorbed moisture causing all the issues above.<br />I am drying it right now at around 90c (cant tell exactly) in a toaster (mini oven with built in air circulation fan) for about 1hr +<br />Should i go 100 ? I dont know if i can get temp exactly since its a kitchen appliance and not a drying unit with sophisticated term-monitoring system like the one came with filastruder.</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Mon, 11 Aug 2014 03:17:44 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62873/#p62873</guid>
		</item>
		<item>
			<title><![CDATA[Re: Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62707/#p62707</link>
			<description><![CDATA[<p>Have you dried the PLA? If so, how?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 09 Aug 2014 12:14:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62707/#p62707</guid>
		</item>
		<item>
			<title><![CDATA[Is there a better feeder screw ?]]></title>
			<link>https://www.soliforum.com/post/62700/#p62700</link>
			<description><![CDATA[<p>I cant get my thing to extrude, it keeps moving pellets around and not pushing them thru unless i press it down with something. (mostly finger)<br />Is there another feeder screw or what ever out there that i can try ?<br />It would go with good rate and then stop, sag and stretch and finally fall out with big blob of PLA.</p><p>ABS pellets that came with the unit were very nice but this PLA i bought&nbsp; has rounded bb&#039;s that just keep on slipping thru the shaft like nothing is pushing it at all.</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Sat, 09 Aug 2014 10:19:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62700/#p62700</guid>
		</item>
	</channel>
</rss>