<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — How to switch from ABS to PLA?]]></title>
		<link>https://www.soliforum.com/topic/7163/how-to-switch-from-abs-to-pla/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/7163/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in How to switch from ABS to PLA?.]]></description>
		<lastBuildDate>Fri, 08 Aug 2014 03:51:57 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/62577/#p62577</link>
			<description><![CDATA[<p>I&#039;ve gotten good at taking my Filastruder apart and back together.&nbsp; I just take the barrel off and soak it in acetone to get all the ABS out.&nbsp; Probably not needed, but it makes for good switches between colors.</p>]]></description>
			<author><![CDATA[null@example.com (milehigh3dII)]]></author>
			<pubDate>Fri, 08 Aug 2014 03:51:57 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62577/#p62577</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/62268/#p62268</link>
			<description><![CDATA[<p>If you have chips in your filament, pull the drill bit out and see where it scratches the tube.<br />Polish the scratched tube area with sand paper and use some grinder to grind off the part that scratches the tube.<br />Dont just grind it off, make it smooth so it would slide across the tube surface rather then scratching it.</p><p>I did it and no more flakes.</p>]]></description>
			<author><![CDATA[null@example.com (tonycstech)]]></author>
			<pubDate>Wed, 06 Aug 2014 09:19:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/62268/#p62268</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61729/#p61729</link>
			<description><![CDATA[<p>Thanks, I will look into getting a melt filter.</p>]]></description>
			<author><![CDATA[null@example.com (icecats)]]></author>
			<pubDate>Fri, 01 Aug 2014 21:06:12 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61729/#p61729</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61728/#p61728</link>
			<description><![CDATA[<p>I&#039;m not a big fan of saying no, but Tim&#039;s filters are CNC machined to precision.&nbsp; It&#039;s money well spent.&nbsp; </p><p>Here&#039;s an in depth discussion:&nbsp; <a href="http://www.soliforum.com/topic/3856/melt-filter-how-to-get-it/">http://www.soliforum.com/topic/3856/mel … to-get-it/</a></p><p>Yes, the printer nozzle.&nbsp; &nbsp;Since 0.4, 0.5, and 0.35 are the most common sized hotends, yupp, melt filter.&nbsp; Clogs are nasty to deal with, I&#039;ve had to clear them too many times.</p>]]></description>
			<author><![CDATA[null@example.com (raykholo)]]></author>
			<pubDate>Fri, 01 Aug 2014 21:04:23 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61728/#p61728</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61727/#p61727</link>
			<description><![CDATA[<p>The other option is to hot pull the nozzle and reach in with needle nose pliers to clean out most of the ABS.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Fri, 01 Aug 2014 20:58:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61727/#p61727</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61726/#p61726</link>
			<description><![CDATA[<p>Thanks for the reply. Is there any way to diy a melt filter? I infer that the .6 nozzle diameter you are referring to is on the printer, correct? Thanks, icecats</p>]]></description>
			<author><![CDATA[null@example.com (icecats)]]></author>
			<pubDate>Fri, 01 Aug 2014 20:57:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61726/#p61726</guid>
		</item>
		<item>
			<title><![CDATA[Re: How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61725/#p61725</link>
			<description><![CDATA[<p>After you finish the initial ABS purge, are you planning to switch over to a nozzle with melt filter?&nbsp; If yes, now is the time to do so.&nbsp; (If you&#039;re running a nozzle smaller than 0.6mm, you should use a melt filter.)&nbsp; </p><p>Once you&#039;ve made the change (if you do) then just start putting PLA pellets in your hopper.&nbsp; Keep the temp at 180 until all the ABS is flushed out.&nbsp; This does take a little while but believe me, you&#039;ll know once all the ABS is out.&nbsp; Natural pla comes out translucent and at 180 degrees, it will be quite thin.&nbsp; Once it&#039;s just PLA coming out, bring your temp down to PLA temps.</p>]]></description>
			<author><![CDATA[null@example.com (raykholo)]]></author>
			<pubDate>Fri, 01 Aug 2014 20:53:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61725/#p61725</guid>
		</item>
		<item>
			<title><![CDATA[How to switch from ABS to PLA?]]></title>
			<link>https://www.soliforum.com/post/61724/#p61724</link>
			<description><![CDATA[<p>Dear Soliforum and Filastruder Community,<br />I have been using my awesome Filastruder for a couple of days, and would now like to switch from extruding ABS to PLA. Does anyone have any tips on switching material? Thanks, icecats</p>]]></description>
			<author><![CDATA[null@example.com (icecats)]]></author>
			<pubDate>Fri, 01 Aug 2014 20:48:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/61724/#p61724</guid>
		</item>