<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Why not Polypropylene?]]></title>
		<link>https://www.soliforum.com/topic/6960/why-not-polypropylene/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6960/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Why not Polypropylene?.]]></description>
		<lastBuildDate>Sat, 12 Jul 2014 09:15:44 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Why not Polypropylene?]]></title>
			<link>https://www.soliforum.com/post/60236/#p60236</link>
			<description><![CDATA[<p>See I would have thought it would have been fine too (coming from a plastic pipe extrusion plant years ago). Formed a nice shell, took less energy to form, cost far less, cooled quicker than our ABS lines, and it smelled so much nicer.</p><p>A shame if that&#039;s the final answer.</p>]]></description>
			<author><![CDATA[null@example.com (exineport)]]></author>
			<pubDate>Sat, 12 Jul 2014 09:15:44 +0000</pubDate>
			<guid>https://www.soliforum.com/post/60236/#p60236</guid>
		</item>
		<item>
			<title><![CDATA[Re: Why not Polypropylene?]]></title>
			<link>https://www.soliforum.com/post/60225/#p60225</link>
			<description><![CDATA[<div class="quotebox"><cite>elmoret wrote:</cite><blockquote><p>Doesn&#039;t extrude well, doesn&#039;t print well. Has been posted here on the forums several times.</p></blockquote></div><p>Ok, thanks for the answer.</p>]]></description>
			<author><![CDATA[null@example.com (EvansRus)]]></author>
			<pubDate>Sat, 12 Jul 2014 04:45:12 +0000</pubDate>
			<guid>https://www.soliforum.com/post/60225/#p60225</guid>
		</item>
		<item>
			<title><![CDATA[Re: Why not Polypropylene?]]></title>
			<link>https://www.soliforum.com/post/60224/#p60224</link>
			<description><![CDATA[<p>Doesn&#039;t extrude well, doesn&#039;t print well. Has been posted here on the forums several times.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 12 Jul 2014 04:42:31 +0000</pubDate>
			<guid>https://www.soliforum.com/post/60224/#p60224</guid>
		</item>
		<item>
			<title><![CDATA[Why not Polypropylene?]]></title>
			<link>https://www.soliforum.com/post/60222/#p60222</link>
			<description><![CDATA[<p>I&#039;m interested in the use of 3d printers for recycling plastic.&nbsp; I&#039;ve been doing some reading about the different types of plastic used for them.&nbsp; I&#039;ve found some information about why HDPE isn&#039;t popular, but why not Polypropylene?&nbsp; It&#039;s common, comes in many different color and is pretty resilient.&nbsp; There must be some good reason why it isn&#039;t popular for 3d printing.&nbsp; Someone please tell me what it is.</p>]]></description>
			<author><![CDATA[null@example.com (EvansRus)]]></author>
			<pubDate>Sat, 12 Jul 2014 03:55:02 +0000</pubDate>
			<guid>https://www.soliforum.com/post/60222/#p60222</guid>
		</item>
	</channel>
</rss>