<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Filament Expanding]]></title>
		<link>https://www.soliforum.com/topic/6823/filament-expanding/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6823/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filament Expanding.]]></description>
		<lastBuildDate>Mon, 30 Jun 2014 22:45:58 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59550/#p59550</link>
			<description><![CDATA[<div class="quotebox"><cite>mangoboy wrote:</cite><blockquote><p>I don&#039;t exactly know what type of ABS it is. It was lying around in our lab, but. I have attached pictures of our setup. We are extruding @ 180 C . Tell me if you need anymore pictures.</p></blockquote></div><p>It&#039;s probably ABS/PC blend.&nbsp; Is it a gritty grey with what looks like chunks of dirt in the extruded plastic?</p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Mon, 30 Jun 2014 22:45:58 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59550/#p59550</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59403/#p59403</link>
			<description><![CDATA[<p>I didn&#039;t build the extruder, someone else did. Thank you for pointing out the issues. I will&nbsp; re-assemble it from scratch. The wooden blocks are there because the wood which the filastruder sits on is lifting from the base. The whole things is embeded into acrylic.</p>]]></description>
			<author><![CDATA[null@example.com (mangoboy)]]></author>
			<pubDate>Thu, 26 Jun 2014 20:50:40 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59403/#p59403</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59389/#p59389</link>
			<description><![CDATA[<p>You didn&#039;t follow the directions on the filament guide, it&#039;s far too far away from the nozzle. There&#039;s dimensions for this in the instructions.</p><p>You also should not have those boards on top of the unit, you&#039;re transferring thrust to the motor for which it is not rated.</p><p>Why didn&#039;t you start with the included ABS that came with the kit? &quot;Random ABS&quot; is not good, it may have undesirable properties.</p><p>EDIT: You also assembled it completely wrong, flange is on the wrong side, spacers are wrong. Did you even look at the instructions?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Thu, 26 Jun 2014 17:12:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59389/#p59389</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59386/#p59386</link>
			<description><![CDATA[<p>I don&#039;t exactly know what type of ABS it is. It was lying around in our lab, but. I have attached pictures of our setup. We are extruding @ 180 C . Tell me if you need anymore pictures.</p>]]></description>
			<author><![CDATA[null@example.com (mangoboy)]]></author>
			<pubDate>Thu, 26 Jun 2014 17:04:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59386/#p59386</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59376/#p59376</link>
			<description><![CDATA[<p>What ABS are you using? Can you post photos of your setup? I have never hard of die swell that significant, it is not normal and indicates something wi wrong with your ABS or your setup. What temperature are you extruding at?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Thu, 26 Jun 2014 16:06:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59376/#p59376</guid>
		</item>
		<item>
			<title><![CDATA[Filament Expanding]]></title>
			<link>https://www.soliforum.com/post/59375/#p59375</link>
			<description><![CDATA[<p>Hello All,</p><p>I built a filastruder kit, and I am trying to get the filament to be 1.75mm in diameter but it ends up expanding to 2.25mm. This will not work with my printer, and I need to fix that. Also, the filament is grainy. I am using ABS pellets. Does anyone have any suggestions?</p><p>-mangoboy</p>]]></description>