<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Print problems]]></title>
		<link>https://www.soliforum.com/topic/6817/print-problems/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6817/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Print problems.]]></description>
		<lastBuildDate>Fri, 27 Jun 2014 14:13:39 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Print problems]]></title>
			<link>https://www.soliforum.com/post/59421/#p59421</link>
			<description><![CDATA[<p>I think you may be on to something.&nbsp; I cannot find an exact temperature setting for the filament anywhere but when my original filament ran out, my printer was set at 215 and I always got good prints, when I started printing with the new filament that is not xyz, the layers would peel away from each other, so I upped the temp with the cartridge resetter to 230.&nbsp; The first couple prints turned out fine with that temp so I thought it was good.&nbsp; I tried last night turning the temp back with the resetter and now I am getting the poor layer bonding again, but the prints look good again.&nbsp; I may have to upgrade firmware to use repetier in order to get my temp to 220 since 215 is just not going to work.&nbsp; Because I got those first couple good prints after temp change, I never thought that may be the problem.</p><p>Thanks</p>]]></description>
			<author><![CDATA[null@example.com (Jaeg)]]></author>
			<pubDate>Fri, 27 Jun 2014 14:13:39 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59421/#p59421</guid>
		</item>
		<item>
			<title><![CDATA[Re: Print problems]]></title>
			<link>https://www.soliforum.com/post/59369/#p59369</link>
			<description><![CDATA[<p>It looks like you&#039;re printing at the wrong temperature.</p><p>What are the temp. specs for the filament you&#039;re using?</p>]]></description>
			<author><![CDATA[null@example.com (tryersol)]]></author>
			<pubDate>Thu, 26 Jun 2014 14:34:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59369/#p59369</guid>
		</item>
		<item>
			<title><![CDATA[Print problems]]></title>
			<link>https://www.soliforum.com/post/59354/#p59354</link>
			<description><![CDATA[<p>I need your guys help in finding my issue, I have tried so many different things to fix this.&nbsp; I am currently running on the G firmware.&nbsp; The printer seems to dip in at certain parts of the print, which causes a wall or other things to not be symetrical with the rest of the print.&nbsp; I even printed the bird bath thinking maybe it was XYZ ware or slicer as I did try w34&#039;s software update to load gcode directly, but this issue was before that.&nbsp; I am attaching some pics of the prints.&nbsp; The birdbath turned out aweful, and the pillars you can see a dip at the base of it, but then its perfect going up from there.&nbsp; This is non-divince filament I am using, could it just be that?&nbsp; I had no warping or issues with it letting loose from the bed.</p>]]></description>
			<author><![CDATA[null@example.com (Jaeg)]]></author>
			<pubDate>Thu, 26 Jun 2014 04:53:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59354/#p59354</guid>