<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Y/X Axis Error]]></title>
		<link>https://www.soliforum.com/topic/6645/yx-axis-error/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6645/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Y/X Axis Error.]]></description>
		<lastBuildDate>Mon, 02 Feb 2015 15:33:39 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/82873/#p82873</link>
			<description><![CDATA[<p>My error 0030 code was due to a short in the x-axis sensor cable assembly. Easy to verify with continuity check w/ multi-meter.<br />Mine was pinched with cable tie on the y-axis carriage and caused a short.<br />X-axis sensor is the 3 red wire harness. Y-axis is 3 orange wire harness. Find on mainboard and follow up to sensor locations.<br />My printer is 1.0A, so colors may be different, but should be easy to identify on mainboard.</p>]]></description>
			<author><![CDATA[null@example.com (mitchlandry)]]></author>
			<pubDate>Mon, 02 Feb 2015 15:33:39 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82873/#p82873</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/82867/#p82867</link>
			<description><![CDATA[<p>I also have an 0030 error - Which means &quot;X-axis movement abnormalities&quot; according to the manual.</p><p>Action (according to manual): Check motor/sensor connections. Check sensor position.</p><p>The problem is obvious - the plate has gone way up, even bending the moving belt. This hinders the extruder from going left on the X-axis.<br />The solution is, however not obvious. I can&#039;t access the menu to pull down the plate. And I can&#039;t find the sensors - exept from the one on the extruder according to a xyzprinting video on the Da Vinci 1.0 (which is almost identical to my Da Vinci 2.0 AiO).</p><p>Any ideas?<br />Thanks.</p>]]></description>
			<author><![CDATA[null@example.com (moph)]]></author>
			<pubDate>Mon, 02 Feb 2015 14:24:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/82867/#p82867</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57978/#p57978</link>
			<description><![CDATA[<div class="quotebox"><cite>NeedsMoarTurbo wrote:</cite><blockquote><div class="quotebox"><cite>mrcobra92 wrote:</cite><blockquote><p>Ok, that got the screen working but now I have a new problem. When I start it up, I still get the buzzing and the lights flashing, but now I get a new error that says &quot;Service Call 0031&quot; which is for the Y axis motor that is working fine, every time I start it up it moves just fine, then spits out that error. If I unplug the Y axis motor, it will almost get to the home screen, then it throws up &quot;Service Call 0030&quot; which is for the X axis motor which is also working just fine as I have seen it move. So I am not sure what is wrong, I highly doubt bother motors have issues.</p></blockquote></div><p>well, can you see or investigate what exactly is making the buzzing noise? do you have a loose belt so the motor is just spinning away and not moving the belt? perhaps you have a problem with an endstop? could be several things I would take a good look around</p></blockquote></div><p>It&#039;s the warning buzzer. I just ended up contacting the seller and am shipping it back for a refund. I am going to just have to wait until a new good deal comes on the market again and hope that one works. I bought this one off ebay, supposedly it was brand new yet it had so manny defects and issues, it looked like it had been dropped off the back of a truck.</p>]]></description>
			<author><![CDATA[null@example.com (mrcobra92)]]></author>
			<pubDate>Thu, 05 Jun 2014 04:25:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57978/#p57978</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57971/#p57971</link>
			<description><![CDATA[<div class="quotebox"><cite>mrcobra92 wrote:</cite><blockquote><p>Ok, that got the screen working but now I have a new problem. When I start it up, I still get the buzzing and the lights flashing, but now I get a new error that says &quot;Service Call 0031&quot; which is for the Y axis motor that is working fine, every time I start it up it moves just fine, then spits out that error. If I unplug the Y axis motor, it will almost get to the home screen, then it throws up &quot;Service Call 0030&quot; which is for the X axis motor which is also working just fine as I have seen it move. So I am not sure what is wrong, I highly doubt bother motors have issues.</p></blockquote></div><p>well, can you see or investigate what exactly is making the buzzing noise? do you have a loose belt so the motor is just spinning away and not moving the belt? perhaps you have a problem with an endstop? could be several things I would take a good look around</p>]]></description>
			<author><![CDATA[null@example.com (NeedsMoarTurbo)]]></author>
			<pubDate>Thu, 05 Jun 2014 04:08:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57971/#p57971</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57939/#p57939</link>
			<description><![CDATA[<p>Ok, that got the screen working but now I have a new problem. When I start it up, I still get the buzzing and the lights flashing, but now I get a new error that says &quot;Service Call 0031&quot; which is for the Y axis motor that is working fine, every time I start it up it moves just fine, then spits out that error. If I unplug the Y axis motor, it will almost get to the home screen, then it throws up &quot;Service Call 0030&quot; which is for the X axis motor which is also working just fine as I have seen it move. So I am not sure what is wrong, I highly doubt bother motors have issues.</p>]]></description>
			<author><![CDATA[null@example.com (mrcobra92)]]></author>
			<pubDate>Wed, 04 Jun 2014 21:13:58 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57939/#p57939</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57922/#p57922</link>
			<description><![CDATA[<p>Try this <a href="http://www.soliforum.com/topic/6495/how-to-repair-the-lcd-easy-fix/">http://www.soliforum.com/topic/6495/how … -easy-fix/</a></p>]]></description>
			<author><![CDATA[null@example.com (heidkampn1)]]></author>
			<pubDate>Wed, 04 Jun 2014 18:23:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57922/#p57922</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57920/#p57920</link>
			<description><![CDATA[<div class="quotebox"><cite>heidkampn1 wrote:</cite><blockquote><p>That&#039;s usually when an error code displays on the screen. Does the screen light up at all?</p></blockquote></div><p>No.</p>]]></description>
			<author><![CDATA[null@example.com (mrcobra92)]]></author>
			<pubDate>Wed, 04 Jun 2014 17:27:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57920/#p57920</guid>
		</item>
		<item>
			<title><![CDATA[Re: Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57919/#p57919</link>
			<description><![CDATA[<p>That&#039;s usually when an error code displays on the screen. Does the screen light up at all?</p>]]></description>
			<author><![CDATA[null@example.com (heidkampn1)]]></author>
			<pubDate>Wed, 04 Jun 2014 17:24:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57919/#p57919</guid>
		</item>
		<item>
			<title><![CDATA[Y/X Axis Error]]></title>
			<link>https://www.soliforum.com/post/57918/#p57918</link>
			<description><![CDATA[<p>Well I just got my printer in the mail, but when I turn it on, I get the buzzing sound and the lights flashing, but now I get a new error that says &quot;Service Call 0031&quot; which is for the Y axis motor that is working fine, every time I start it up it moves just fine, then spits out that error. If I unplug the Y axis motor, it will almost get to the home screen, then it throws up &quot;Service Call 0030&quot; which is for the X axis motor which is also working just fine as I have seen it move. So I am not sure what is wrong, I highly doubt bother motors have issues.</p>]]></description>