<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Blobby Perimeters after E3D 0.6mm Install]]></title>
		<link>https://www.soliforum.com/topic/6611/blobby-perimeters-after-e3d-06mm-install/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6611/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Blobby Perimeters after E3D 0.6mm Install.]]></description>
		<lastBuildDate>Mon, 02 Jun 2014 02:22:39 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Blobby Perimeters after E3D 0.6mm Install]]></title>
			<link>https://www.soliforum.com/post/57698/#p57698</link>
			<description><![CDATA[<p>I just started the print over at a slower speed and so far, it looks like the problem is solved.&nbsp; I think I discovered an upper limit to the volume throughput on the E3D.&nbsp; It didn&#039;t seem that fast at first because I used to run at 150 mm/s and never had issues.&nbsp; But that was with a 0.35mm nozzle.&nbsp; Now with the E3D setup, I have a 0.6mm nozzle, 0.75mm width and printing at 0.5mm layer height, the throughput is considerably higher, even at slower movement speed.&nbsp; I will have to experiment to find the exact speed at which the output starts blobbing.</p><p>This is a bit of a bummer because I bought the E3D and 0.6mm nozzle so that I could print at insane speeds with low (but good enough) resolution.&nbsp; Now I will have to limit my speed to somewhere around 80mm/s.</p>]]></description>
			<author><![CDATA[null@example.com (ne14pez)]]></author>
			<pubDate>Mon, 02 Jun 2014 02:22:39 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57698/#p57698</guid>
		</item>
		<item>
			<title><![CDATA[Re: Blobby Perimeters after E3D 0.6mm Install]]></title>
			<link>https://www.soliforum.com/post/57687/#p57687</link>
			<description><![CDATA[<p>Settings seem ok, other than temp may be a touch high (esp for the wide-bore nozzle)? I get away with about 230C most of the time with an 0.4mm nozzle (albeit only running at c. 60 mm/s), this varies between people (and preference) and your numbers aren&#039;t silly.</p><p>That said, definitely shouldn&#039;t be any burning like that. Have you updated the firmware to reflect the new sensor for the E3D, or did you reuse the old sensor? Is the sensor installed securely?</p><p>The free extrusion swelling, and that being different depending on speed is pretty normal: it&#039;s called &quot;die swell&quot; - the filastruder peeps on this forum discuss it in great detail. The volume coming out is dependent on the volume going in, so this is probably not a problem for you.</p><p>Have you calibrated the steps-per-mm again for the new setup (didn&#039;t change much when I put my E3D on), and done a wall-thickness calibration again? Could be a wee bit of overextrusion.</p><p>Apologies, lots of questions, but lots of possible causes! <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (grob)]]></author>
			<pubDate>Mon, 02 Jun 2014 01:42:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57687/#p57687</guid>
		</item>
		<item>
			<title><![CDATA[Re: Blobby Perimeters after E3D 0.6mm Install]]></title>
			<link>https://www.soliforum.com/post/57685/#p57685</link>
			<description><![CDATA[<p>I just discovered something.&nbsp; I was playing with just extruding over thin air and if I extrude faster than about 300 mm/s, the bead swells in diameter.&nbsp; If I extrude slowly, it comes out at 0.6mm (same as nozzle), but if I speed it up to say 500 mm/s, it swells to over 1mm in diameter!&nbsp; Is this causing the blobbing problem?&nbsp; Do I have to just limit the extrusion speed?</p>]]></description>
			<author><![CDATA[null@example.com (ne14pez)]]></author>
			<pubDate>Mon, 02 Jun 2014 01:26:51 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57685/#p57685</guid>
		</item>
		<item>
			<title><![CDATA[Blobby Perimeters after E3D 0.6mm Install]]></title>
			<link>https://www.soliforum.com/post/57680/#p57680</link>
			<description><![CDATA[<p>As you can see in the attached picture, my perimeters are really blobby and burnt in some places.&nbsp; The first layer prints perfectly, but subsequent layers get messed up.&nbsp; Solid fill and hex fill both print fine on all layers.&nbsp; I&#039;m printing at 100 mm/s, with the first layer at 60%.&nbsp; Retraction is 2mm at 70 mm/s.&nbsp; Temp. is 250C/245C.&nbsp; What am I doing wrong?</p>]]></description>