<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — why does this happen? please help]]></title>
		<link>https://www.soliforum.com/topic/6578/why-does-this-happen-please-help/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6578/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in why does this happen? please help.]]></description>
		<lastBuildDate>Mon, 02 Jun 2014 10:23:20 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57714/#p57714</link>
			<description><![CDATA[<div class="quotebox"><cite>ronsii wrote:</cite><blockquote><p>I am surprised by the evenness of the repetition... have you tuned the stepper voltages?</p></blockquote></div><br /><p>No, I haven&#039;t touch anything to the stepper voltage. Its as is from solidoodle.</p>]]></description>
			<author><![CDATA[null@example.com (iiinsaiii)]]></author>
			<pubDate>Mon, 02 Jun 2014 10:23:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57714/#p57714</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57532/#p57532</link>
			<description><![CDATA[<p>I am surprised by the evenness of the repetition... have you tuned the stepper voltages?</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Sat, 31 May 2014 18:50:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57532/#p57532</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57518/#p57518</link>
			<description><![CDATA[<p>Just a guess: slight over extrusion and the bed is slightly higher on that end.&nbsp; I would also guess that began on the first layer and amplified all the way up.</p>]]></description>
			<author><![CDATA[null@example.com (wardjr)]]></author>
			<pubDate>Sat, 31 May 2014 14:43:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57518/#p57518</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57504/#p57504</link>
			<description><![CDATA[<p>Yes it worked! I raised the temp to 215 and added a top enclosure, plus lower the lay height to&nbsp; .2936. I came out fine, except for the waves on one side of the wall. That wall side was facing the front and I don&#039;t understand why are there waves. The waves stick out more from the inside. Any ideas what&#039;s causing it?</p>]]></description>
			<author><![CDATA[null@example.com (iiinsaiii)]]></author>
			<pubDate>Sat, 31 May 2014 10:49:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57504/#p57504</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57419/#p57419</link>
			<description><![CDATA[<p>Either switch to PLA, or fully enclose the printer. ABS is meant to be an injection molding plastic, meaning it shrinks slightly when cooling.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Fri, 30 May 2014 15:18:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57419/#p57419</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57413/#p57413</link>
			<description><![CDATA[<p>Even if you come up with a temporary top (Four triangles of cardboard) that will help retain the heat.&nbsp; Part of what you&#039;re dealing with is shrinkage from uneven or to much cooling.&nbsp; The other thing your dealing with is the fact that SD uses a standard thread instead of metric thread on the Z-Rod.&nbsp; This is where the layer height of .2963 helps out but doesn&#039;t totally fix the problem.<br />The other thing you can do is try some different profile settings as far as perimeters and infill goes.</p>]]></description>
			<author><![CDATA[null@example.com (wardjr)]]></author>
			<pubDate>Fri, 30 May 2014 14:41:40 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57413/#p57413</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57412/#p57412</link>
			<description><![CDATA[<p>Hi, </p><p>I did enclose the fame of the solidoodle, the only thing I didn&#039;t do was add a cover to the top. And I&#039;ve been running it hotter,&nbsp; I had it at 210 the first time and it still didn&#039;t work.</p>]]></description>
			<author><![CDATA[null@example.com (iiinsaiii)]]></author>
			<pubDate>Fri, 30 May 2014 14:33:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57412/#p57412</guid>
		</item>
		<item>
			<title><![CDATA[Re: why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57411/#p57411</link>
			<description><![CDATA[<p>Yep, That really sucks...<br />Try using a layer height of .2963 lots of posts on hear about layer separation.<br />Also hotter filament is better for this situation and if your printer isn&#039;t enclosed that would help too (even the top should be enclosed).<br />Welcome to the forum.</p>]]></description>
			<author><![CDATA[null@example.com (wardjr)]]></author>
			<pubDate>Fri, 30 May 2014 14:23:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57411/#p57411</guid>
		</item>
		<item>
			<title><![CDATA[why does this happen? please help]]></title>
			<link>https://www.soliforum.com/post/57410/#p57410</link>
			<description><![CDATA[<p>Hi, I&#039;m new here and this is my first post.&nbsp; I have the solidoodle 2 Pro that I got a few months ago, I&#039;ve printed a few things that came out fine. I calibrated slicer and it works fine. But every time I try to print this large part I&#039;ve been running into this problem. I&#039;ve been trying to print out this project box for work, but it keeps splitting round one end of the frame and I don&#039;t know why. I change the temp on the extruder from 210 down to 190 and the bed I have it at 100. This takes over 5 hours to print at .3mm. And its driving me crazy. Added all the filament I&#039;ve wasted trying to print this. </p><p>Please help </p><p>Please look at the pictures I posted</p>]]></description>