<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Lil test in smoothing PLA]]></title>
		<link>https://www.soliforum.com/topic/6456/lil-test-in-smoothing-pla/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6456/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Lil test in smoothing PLA.]]></description>
		<lastBuildDate>Thu, 26 Jun 2014 18:12:50 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59395/#p59395</link>
			<description><![CDATA[<p>I used some gloss mod podge spray to make them shiney and that worked pretty well. At that point they almost look acetone smoothed but not quite.</p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Thu, 26 Jun 2014 18:12:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59395/#p59395</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59226/#p59226</link>
			<description><![CDATA[<p>As another note. I didn&#039;t do any sanding for these tests so far</p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 24 Jun 2014 12:20:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59226/#p59226</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59185/#p59185</link>
			<description><![CDATA[<p>Note that it does not leave them super shiney like acetone smoothing. Though it does seem to retain some shinyness if the material was.</p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 24 Jun 2014 00:55:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59185/#p59185</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59183/#p59183</link>
			<description><![CDATA[<p>A second time being smoothed showed some more improvements but not a great amount. Still not at the level of acetone smoothing but not bad either.</p><p><span class="postimg"><img src="http://i.imgur.com/jCBYLAH.jpg" alt="http://i.imgur.com/jCBYLAH.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 24 Jun 2014 00:49:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59183/#p59183</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59181/#p59181</link>
			<description><![CDATA[<p>Very cool. Seems like you are ahead of the curve in PLA smoothing provided my personal research.<br />Keep it up!</p>]]></description>
			<author><![CDATA[null@example.com (AZERATE)]]></author>
			<pubDate>Tue, 24 Jun 2014 00:16:12 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59181/#p59181</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/59172/#p59172</link>
			<description><![CDATA[<p>Here is 4 more PLA items smoothed with MEK Substitute.&nbsp; Less time was better. Once I saw the vapors I kept it in 20-30 seconds.</p><p><span class="postimg"><img src="http://i.imgur.com/XrCxuXG.jpg" alt="http://i.imgur.com/XrCxuXG.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Mon, 23 Jun 2014 22:47:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/59172/#p59172</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/57068/#p57068</link>
			<description><![CDATA[<p>I do hope to play with this some more soon, try with it being in less time to hopefully avoid the white marks. I was leaving it in after the vapors started maybe a minute; So that maybe too long.</p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 27 May 2014 12:24:51 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57068/#p57068</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/57066/#p57066</link>
			<description><![CDATA[<p>Wow! This seems promising. I wonder why more people are not pushing this info. Nice work!</p>]]></description>
			<author><![CDATA[null@example.com (machinistjoe)]]></author>
			<pubDate>Tue, 27 May 2014 11:30:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/57066/#p57066</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/56691/#p56691</link>
			<description><![CDATA[<p>Better pic of the &quot;after&quot;. Note the whiteish discoloration at the base, I think I need to leave it in less time.</p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5348&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=5348&amp;amp;download=0" /></span></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 20 May 2014 23:28:31 +0000</pubDate>
			<guid>https://www.soliforum.com/post/56691/#p56691</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/56687/#p56687</link>
			<description><![CDATA[<p>Ok this time only once through. Presto cooker at 350. Enough MEK for a light cover of the bottom. Left in a minute after I saw the vapors. I may want to try 30 seconds next time since I&#039;m getting areas of white as spots.</p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5345&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=5345&amp;amp;download=0" /></span></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Tue, 20 May 2014 23:21:27 +0000</pubDate>
			<guid>https://www.soliforum.com/post/56687/#p56687</guid>
		</item>
		<item>
			<title><![CDATA[Re: Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/56571/#p56571</link>
			<description><![CDATA[<p>Very cool! Last I read THF was just about the only option, so this quite nice.</p>]]></description>
			<author><![CDATA[null@example.com (AZERATE)]]></author>
			<pubDate>Mon, 19 May 2014 13:33:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/56571/#p56571</guid>
		</item>
		<item>
			<title><![CDATA[Lil test in smoothing PLA]]></title>
			<link>https://www.soliforum.com/post/56570/#p56570</link>
			<description><![CDATA[<p>First off I found this blog entry with smoothing PLA <a href="http://www.printedsolid.com/smoothpla/">http://www.printedsolid.com/smoothpla/</a> and tried to replicate this. </p><p>Things to correct for next test<br />- I ran this through the process twice, next time only once at first<br />- More sanding needed before smoothing<br />- I got impatient, and turned the temp all the way up. I probably shouldn&#039;t of had</p><p>Notes:<br />- This PLA chess peice had some pretty bad over hangs in some parts. Wasn&#039;t the M.E.Ks substitutes fault<br />- I used the &quot;Presto cooker&quot;<br />- I made sure I did this outside<br />- Seems about as noxious as Acetone<br />- I went to the home depot and got Klean Strip MEK Substitute<br />- Treated it like a acetone vapor treatment<br />- I used purple translucent PLA for the print</p><p>Results:<br />- Took a lil longer for the MEK Substiute to vaporize, but not too much. Maybe goes at a higher temp<br />- Smoothed less then actone and ABS, but still a decent amount<br />- Some white areas created white lines but I think that is quite possibly my mistake on how I did the experient and running it in twice<br />- Tactile-wise&nbsp; It seemed only a lil soft to the touch after 5 minutes. Less so then with ABS</p><br /><p>I hope to try this again soonish (I have a E3D to install soon though! <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> ))</p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5329&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=5329&amp;amp;download=0" /></span></p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=5330&amp;download=0" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=5330&amp;amp;download=0" /></span></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Mon, 19 May 2014 12:49:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/56570/#p56570</guid>
		</item>
	</channel>
</rss>