<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Need Slicer ABS Filliment defaults]]></title>
		<link>https://www.soliforum.com/topic/6367/need-slicer-abs-filliment-defaults/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6367/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Need Slicer ABS Filliment defaults.]]></description>
		<lastBuildDate>Wed, 07 May 2014 15:23:19 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Need Slicer ABS Filliment defaults]]></title>
			<link>https://www.soliforum.com/post/55882/#p55882</link>
			<description><![CDATA[<p>Thanks. I&#039;ll try those settings when I get home <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></description>
			<author><![CDATA[null@example.com (LdyMox)]]></author>
			<pubDate>Wed, 07 May 2014 15:23:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55882/#p55882</guid>
		</item>
		<item>
			<title><![CDATA[Re: Need Slicer ABS Filliment defaults]]></title>
			<link>https://www.soliforum.com/post/55850/#p55850</link>
			<description><![CDATA[<p>Start with a filament diameter of 1.75mm and extrusion multiplier of about 0.80 (0.80-1.00 is pretty normal)<br />I use an E3D hot end, so my temps are 240 first layer / 230 the rest, but for a stock hotend start around 210.<br />I&#039;m not a huge believer in accurate measurement of filament diameter, but certainly do a wall thickness calibration for the extrusion multiplier.</p>]]></description>
			<author><![CDATA[null@example.com (grob)]]></author>
			<pubDate>Wed, 07 May 2014 04:05:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55850/#p55850</guid>
		</item>
		<item>
			<title><![CDATA[Need Slicer ABS Filliment defaults]]></title>
			<link>https://www.soliforum.com/post/55823/#p55823</link>
			<description><![CDATA[<p>In slic3r (SD2) under the filament setting referring to Diameter and Extrusion Multiplier for ABS. What defaults to people have? I was messing with the settings and I think I totally messed them up.</p>]]></description>