		<title><![CDATA[SoliForum - 3D Printing Community — Filament is not extruding during printing, at all.]]></title>
		<link>https://www.soliforum.com/topic/6293/filament-is-not-extruding-during-printing-at-all/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6293/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filament is not extruding during printing, at all..]]></description>
		<lastBuildDate>Sun, 04 May 2014 04:41:19 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55631/#p55631</link>
			<description><![CDATA[<p>From your video #mov002, I think you have a sticking problem,<br />or the gap between the nozzle and the bed is too big, if you don&#039;t<br />know where is a Z-tab or an adjusting screw to calibrate the heating<br />bed(bridge), I don&#039;t think you level the print bed properly, so if <br />you can get the right gap(somebody inserts a metro card to measure it),<br />and use the hairspray, you will solve this problem. Just try, let us know <br />the result.</p>]]></description>
			<author><![CDATA[null@example.com (AOYOU3D)]]></author>
			<pubDate>Sun, 04 May 2014 04:41:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55631/#p55631</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55625/#p55625</link>
			<description><![CDATA[<p>Could you please read my previous posts about this problem before you decide to post.. I&#039;ve already said I don&#039;t have any issues with sticking when this issue isn&#039;t a problem.</p><p>And just for re-clarification for those that are new to this post:</p><p>-My print bed is level<br />-My extruder is manually extruding<br />-My prints stick when this is not a problem.<br />-In my videos the filament you see being used is what leaks out during printing<br />-My z-axis is positioned low on purpose for the video so it does not need to be adjusted.<br />-I&#039;m using STLs and codes I&#039;ve used previously so I know they print.</p>]]></description>
			<author><![CDATA[null@example.com (7DSins)]]></author>
			<pubDate>Sun, 04 May 2014 01:36:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55625/#p55625</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55577/#p55577</link>
			<description><![CDATA[<p>If you think the gap between of the nozzle and the bed is OK, <br />when the bed temp. reached to 95-105C, you can put some <br />hair spray on the bed to hold your prints.</p>]]></description>
			<author><![CDATA[null@example.com (AOYOU3D)]]></author>
			<pubDate>Sat, 03 May 2014 02:51:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55577/#p55577</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55492/#p55492</link>
			<description><![CDATA[<p>-If you look at my other video (#1 I think it is) you&#039;ll see me feeding the filament through the extruder. It changes from black to green eventually. </p><p>-my print bed is level</p><p>- the z-axis is purposefully set high (or low, which ever you prefer) in my video to show that it&#039;s not extruding properly.</p><p>-The model I&#039;m attempting to print I&#039;ve done with both an STL and a G-code.</p>]]></description>
			<author><![CDATA[null@example.com (7DSins)]]></author>
			<pubDate>Fri, 02 May 2014 03:30:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55492/#p55492</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55486/#p55486</link>
			<description><![CDATA[<p>7Dsins,</p><p>From your video, the extruder with filament is working very well,<br /> it seems the gap between of the nozzle and the bed is not too close,<br />it is too far, when the nozzle is moving, just pulling the printed lines up, <br />so you can let nozzle stops at the home position, then you can loosen the 3<br />springs by turning the wing nuts underneath bed bridge, decrease the gap.<br />If your bed is leveled perfectly, you don&#039;t want touch 3 springs, you can<br />turn the M3 screw(with a black printed knob) on the Z-tab, it is used with<br />a limit switch to control the home position of the bed bridge(Z-UP-DOWN <br />direction).<br />Just try, very small problem.</p>]]></description>
			<author><![CDATA[null@example.com (AOYOU3D)]]></author>
			<pubDate>Fri, 02 May 2014 02:49:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55486/#p55486</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55476/#p55476</link>
			<description><![CDATA[<p>Have you drawn a sharpie mark on the face of the filament extruder gear that is visible when printing? this way you will be able to see if the stepper is being commanded to extrude filament or not by the slicing software.</p><p>The model you are trying to print that was printed before.... are you printing the actual gcode file that was used before or the stl?</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Fri, 02 May 2014 01:31:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55476/#p55476</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55465/#p55465</link>
			<description><![CDATA[<p>Okay, so after finally getting some time to fiddle with my printer again I adjusted the z-axis and it&#039;s still not extruding filament.</p><p>I&#039;d also like to point out that contacting Solidoodle support is even more frustrating then trying to fix the printer.. Not the best technical support I&#039;ve seen.. probably one of the worst.. But mini-rants caused by frustration aside..</p><p> A third video has been posted on my signature of the current problem I&#039;m facing. I&#039;m still able to extrude the filament manually but when I hit print it&#039;s not coming out as it should. Dry run is not enabled, settings for .1 have not been altered, the z-axis is set a little low on purpose to show what I&#039;m talking about a little easier, and I&#039;m using a model that I&#039;ve printed before so g-codes have not been altered.</p><p>Edit after seeing the picture offered: Yes I found that out after looking all over for the z-axis on my SD4. I was very confused as to where it could be then my friend pointed that out and how it was sitting over a censor on the print bed. So lets all make a note of that shall we!? <img src="https://www.soliforum.com/img/smilies/big_smile.png" width="15" height="15" alt="big_smile" /> the SD4 has a dial for it&#039;s z-axis instead of an adjustable bolt.</p>]]></description>
			<author><![CDATA[null@example.com (7DSins)]]></author>
			<pubDate>Thu, 01 May 2014 22:43:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55465/#p55465</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55322/#p55322</link>
			<description><![CDATA[<p>Excellent, and you can adjust it with the case on too.</p>]]></description>
			<author><![CDATA[null@example.com (ggunners)]]></author>
			<pubDate>Tue, 29 Apr 2014 20:41:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55322/#p55322</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55313/#p55313</link>
			<description><![CDATA[<p>This is what I use to adjust the z-axis on mine, sorry about the quality is phone pic whilst it was printing</p>]]></description>
			<author><![CDATA[null@example.com (envisaged)]]></author>
			<pubDate>Tue, 29 Apr 2014 19:22:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55313/#p55313</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55300/#p55300</link>
			<description><![CDATA[<p>For us that don&#039;t have an SD4, any pictures of the z adjustment?</p>]]></description>
			<author><![CDATA[null@example.com (ggunners)]]></author>
			<pubDate>Tue, 29 Apr 2014 14:20:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55300/#p55300</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55298/#p55298</link>
			<description><![CDATA[<p>I have a SD4 too, my understanding is that to adjust the Z axis you use the big black wheel at the back of the case if you look it is directly above the limit switch, sorry not more help than that as I’m new to this too <img src="https://www.soliforum.com/img/smilies/yikes.png" width="15" height="15" alt="yikes" />)</p>]]></description>
			<author><![CDATA[null@example.com (envisaged)]]></author>
			<pubDate>Tue, 29 Apr 2014 12:05:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55298/#p55298</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55254/#p55254</link>
			<description><![CDATA[<div class="quotebox"><cite>7DSins wrote:</cite><blockquote><p>I don&#039;t have issues with sticking, if you look closely at the printing video you&#039;ll see it&#039;s been scratched up with sandpaper (another trick for sticking that I found people doing), that&#039;s helped things stick rather well up until now. I have no idea why it wasn&#039;t sticking this time around but that&#039;s not really my current problem sadly.</p></blockquote></div><p>Sorry...I missed that one.</p><div class="quotebox"><cite>7DSins wrote:</cite><blockquote><p>I&#039;ve looked all over my solidoodle 4 and can&#039;t find the z-offset that&#039;s outlined in the solidoodle videos. Is it in a different place on 4 then it is on the others?</p></blockquote></div><p>It is that little printed bracket with a M3 bolt found immediately to the left of your unthreaded z rods. This can easily be adjusted with the M3 allen wrench that came with your doodle.</p><div class="quotebox"><cite>7DSins wrote:</cite><blockquote><p>Thank you for all the help you&#039;ve been giving so far, this being my first printer the problems I&#039;ve been having with it have been pretty frustrating.</p></blockquote></div><p>We&#039;ve all been there. Have patience, young grasshopper. <img src="https://www.soliforum.com/img/smilies/big_smile.png" width="15" height="15" alt="big_smile" /></p>]]></description>
			<author><![CDATA[null@example.com (AZERATE)]]></author>
			<pubDate>Mon, 28 Apr 2014 22:06:34 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55254/#p55254</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55252/#p55252</link>
			<description><![CDATA[<p>I don&#039;t have issues with sticking, if you look closely at the printing video you&#039;ll see it&#039;s been scratched up with sandpaper (another trick for sticking that I found people doing), that&#039;s helped things stick rather well up until now. I have no idea why it wasn&#039;t sticking this time around but that&#039;s not really my current problem sadly. </p><p>I&#039;ve looked all over my solidoodle 4 and can&#039;t find the z-offset that&#039;s outlined in the solidoodle videos. Is it in a different place on 4 then it is on the others? </p><p>Side note: Thank you for all the help you&#039;ve been giving so far, this being my first printer the problems I&#039;ve been having with it have been pretty frustrating.</p>]]></description>
			<author><![CDATA[null@example.com (7DSins)]]></author>
			<pubDate>Mon, 28 Apr 2014 21:16:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55252/#p55252</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55250/#p55250</link>
			<description><![CDATA[<div class="quotebox"><cite>7DSins wrote:</cite><blockquote><p>(because for some reason it&#039;s not letting me post the links in this forum)</p></blockquote></div><p>You need to have (I believe) 20 posts before posting links.</p><p>You are certainly having an issue with adhesion, though. Is this the first print you&#039;ve tried? <br />Regardless, I agree with ggunners for glue, hairspray, or slurry.<br />I, as most users on here, recommend glass/mirror bed over your kapton and spray a little super extra hold hairspray...no more stick issues. I never could get a successful print on kapton.<br />And while you want the nozzle close to the bed for a fat and flat first layer, you do not want the nozzle to &quot;kiss&quot; the bed or you will have the issues ggunners mentions.</p>]]></description>
			<author><![CDATA[null@example.com (AZERATE)]]></author>
			<pubDate>Mon, 28 Apr 2014 20:53:26 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55250/#p55250</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filament is not extruding during printing, at all.]]></title>
			<link>https://www.soliforum.com/post/55248/#p55248</link>
			<description><![CDATA[<p>Obviously, it is not sticking well. Increase the stickage. There are many options, hairspray, glue stick, ABS slurry. </p><p>Also, it looks like your z-height adjustment screw is a little too close to the bed. If it is too close to the bed, nothing comes out because there is no space for the filament and it stays inside the barrel. Increase the 1st layer space using the z height screw a very tiny amount until you get a good squished layer.</p>]]></description>
			<author><![CDATA[null@example.com (ggunners)]]></author>
			<pubDate>Mon, 28 Apr 2014 20:20:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55248/#p55248</guid>
		</item>