		<title><![CDATA[SoliForum - 3D Printing Community — Extruding vs Printing Temperature]]></title>
		<link>https://www.soliforum.com/topic/6281/extruding-vs-printing-temperature/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6281/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Extruding vs Printing Temperature.]]></description>
		<lastBuildDate>Mon, 28 Apr 2014 16:16:29 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link>https://www.soliforum.com/post/55234/#p55234</link>
			<description><![CDATA[<p>I may be off on this.&nbsp; I get dark spots on my prints sometimes too.&nbsp; It&#039;s kind of frustrating.&nbsp; I think mine come from residue on the outside of the nozzle from where I had a failed print and the head plowed through some plastic.&nbsp; It&#039; seems to help if I clean it up some.</p>]]></description>
			<author><![CDATA[null@example.com (bbriggsgeek)]]></author>
			<pubDate>Mon, 28 Apr 2014 16:16:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55234/#p55234</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link>https://www.soliforum.com/post/55170/#p55170</link>
			<description><![CDATA[<p>Hi Tim!<br />This is the one that I am usnig: LG HF380 - Melt Temperature (210~240) / Melt Flow Rate (43). Using a 0.35mm RepRap nozzle to extrude 3mm filament.</p>]]></description>
			<author><![CDATA[null@example.com (henriquesv)]]></author>
			<pubDate>Sun, 27 Apr 2014 11:33:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55170/#p55170</guid>
		</item>
		<item>
			<title><![CDATA[Re: Extruding vs Printing Temperature]]></title>
			<link>https://www.soliforum.com/post/55141/#p55141</link>
			<description><![CDATA[<p>Really too many variables to say here. We don&#039;t know what ABS resin you&#039;re using, or what hot end you&#039;re using. Finding ideal printing temperature is a bit of trial and error.</p><p>I extrude MG94 ABS at 187C, and print it at 205C on a Solidoodle hot end.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 26 Apr 2014 16:10:31 +0000</pubDate>
			<guid>https://www.soliforum.com/post/55141/#p55141</guid>
		</item>
		<item>
			<title><![CDATA[Extruding vs Printing Temperature]]></title>
			<link>https://www.soliforum.com/post/55134/#p55134</link>
			<description><![CDATA[<p>Hi!<br />I&#039;ve been extruding ABS for some time already. For the ABS that I am using I set extrusion to 180ºC. But I still didn&#039;t get the proper temperature for 3D Printing. Have you guys reached any relation between extruding and printing?</p><p>For instance, while printing at 215ºC the melt flow seems right, but once in a while I get burned spots.</p><p>Any ideas on this one?</p><p>Thanks!</p>]]></description>