<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Importance of grinding of lips of pipe nipple]]></title>
		<link>https://www.soliforum.com/topic/6197/importance-of-grinding-of-lips-of-pipe-nipple/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6197/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Importance of grinding of lips of pipe nipple.]]></description>
		<lastBuildDate>Sat, 19 Apr 2014 00:05:06 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Importance of grinding of lips of pipe nipple]]></title>
			<link>https://www.soliforum.com/post/54482/#p54482</link>
			<description><![CDATA[<p>Less important on v1.4 than previous versions. Assuming its a 1.4, you&#039;re probably fine.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 19 Apr 2014 00:05:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54482/#p54482</guid>
		</item>
		<item>
			<title><![CDATA[Importance of grinding of lips of pipe nipple]]></title>
			<link>https://www.soliforum.com/post/54481/#p54481</link>
			<description><![CDATA[<p>I am lazy and don&#039;t want to introduce more metal particles into the system - how important is it to grind away the lip on the inside of the pipe? Certainly it can&#039;t be all that important on the motor end at least, or is it?<br />The ridge is nice and smooth and is barely felt with a finger.</p>]]></description>