<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Questions about PET]]></title>
		<link>https://www.soliforum.com/topic/6111/questions-about-pet/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/6111/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Questions about PET.]]></description>
		<lastBuildDate>Tue, 15 Apr 2014 15:23:04 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Questions about PET]]></title>
			<link>https://www.soliforum.com/post/54245/#p54245</link>
			<description><![CDATA[<p>Same seller is preparing a grab-box of plastics for me.&nbsp; Nylon, HDPE, PP, and two other types of PET.&nbsp; Yay!</p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Tue, 15 Apr 2014 15:23:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54245/#p54245</guid>
		</item>
		<item>
			<title><![CDATA[Re: Questions about PET]]></title>
			<link>https://www.soliforum.com/post/54190/#p54190</link>
			<description><![CDATA[<p>The seller spontaneously refunded me half my purchase price, without me asking.&nbsp; Hella awesome considering I was treating it as R&amp;D.&nbsp; Not sure if you&#039;re reading this Ryan but thanks dude <img src="https://www.soliforum.com/img/smilies/cool.png" width="15" height="15" alt="cool" /></p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Mon, 14 Apr 2014 21:04:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54190/#p54190</guid>
		</item>
		<item>
			<title><![CDATA[Re: Questions about PET]]></title>
			<link>https://www.soliforum.com/post/54171/#p54171</link>
			<description><![CDATA[<p>Updates on PET:</p><p>I had a lot of problems with it so far.&nbsp; I still got groaning and popping from the machine at 175C, so I tried 215C.&nbsp; It flowed better, but after several hours I only had a meter of filament, and it was obviously carbonizing.&nbsp; I removed the nozzle and the pellets had made it all the way to the end, encased in a matrix of burnt PET goo.</p><p>I&#039;m going to leave the rest of this up to Taulman.&nbsp; If anyone wants the remaining pellets (probably 4.5lbs worth) they&#039;re yours for shipping.</p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Mon, 14 Apr 2014 13:53:22 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54171/#p54171</guid>
		</item>
		<item>
			<title><![CDATA[Re: Questions about PET]]></title>
			<link>https://www.soliforum.com/post/54106/#p54106</link>
			<description><![CDATA[<p>Did you do any drying to the pellets before extruding?</p><p>have you tried printing the milky filament? it might go clear when you print it.</p>]]></description>
			<author><![CDATA[null@example.com (redback)]]></author>
			<pubDate>Sun, 13 Apr 2014 04:44:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54106/#p54106</guid>
		</item>
		<item>
			<title><![CDATA[Re: Questions about PET]]></title>
			<link>https://www.soliforum.com/post/54018/#p54018</link>
			<description><![CDATA[<p>I have a datasheet!</p><p><a href="http://ws.eastman.com/ProductCatalogApps/PageControllers/ProdDatasheet_PC.aspx?Product=71063602&amp;sCategoryName=Generic">http://ws.eastman.com/ProductCatalogApp … me=Generic</a></p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Fri, 11 Apr 2014 21:07:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/54018/#p54018</guid>
		</item>
		<item>
			<title><![CDATA[Questions about PET]]></title>
			<link>https://www.soliforum.com/post/53927/#p53927</link>
			<description><![CDATA[<p>(haven&#039;t gotten around to the ballistic nylon yet...trying PET first)</p><p>I got <a href="http://cgi.ebay.com/ws/eBayISAPI.dll?ViewItem&amp;item=201046272675">this stuff</a> from eBay, and while I&#039;m waiting for details from the seller for Melt Flow Index, I had a question about the melting temperature vs. what I should be filastruding at.</p><p>The pellets are strangely white, which is what the auction said.&nbsp; He said they turn clear when run hot enough.&nbsp; He also says the melting temperature is ~ 250C.&nbsp; Now, 230C is what I print Taulman PET at, which does turn out approximately water clear.&nbsp; I know that Taulman PET is a different blend, and I&#039;m thinking the 250C in the auction is for injection molding which I&#039;m not sure applies to us.</p><p>I tried extruding at 150C which was a bad idea, so I upped it to 175C.&nbsp; The plastic right out of the nozzle was clear, but cooled to a milk jug white, just like HDPE.&nbsp; It was also very slow, which is why I&#039;m inquiring about MFI.</p><p>Ideas on what I should be trying to extrude this at?</p>]]></description>
			<author><![CDATA[null@example.com (insta)]]></author>
			<pubDate>Thu, 10 Apr 2014 16:49:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/53927/#p53927</guid>
		</item>