<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — extruder crashes on print end with with repetier]]></title>
		<link>https://www.soliforum.com/topic/5969/extruder-crashes-on-print-end-with-with-repetier/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5969/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in extruder crashes on print end with with repetier.]]></description>
		<lastBuildDate>Wed, 26 Mar 2014 19:40:38 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: extruder crashes on print end with with repetier]]></title>
			<link>https://www.soliforum.com/post/53015/#p53015</link>
			<description><![CDATA[<p>I have found the culprit setting in Printer Settings:&nbsp; Go to Park position after job/kill.</p><p>I have used solidoodle&#039;s settings (no upgrades to my printer firmware), and somehow the thing subtracts 159 from the Park value in the X coordinate.&nbsp; I disabled the parking for the time being, but I haven&#039;t decided what values I should use to be sure that my extruder won&#039;t crash.</p>]]></description>
			<author><![CDATA[null@example.com (driggers)]]></author>
			<pubDate>Wed, 26 Mar 2014 19:40:38 +0000</pubDate>
			<guid>https://www.soliforum.com/post/53015/#p53015</guid>
		</item>
		<item>
			<title><![CDATA[Re: extruder crashes on print end with with repetier]]></title>
			<link>https://www.soliforum.com/post/52951/#p52951</link>
			<description><![CDATA[<p>Checked.&nbsp; Not there.&nbsp; And not in any of the number scripts, or anything in that menu.</p>]]></description>
			<author><![CDATA[null@example.com (driggers)]]></author>
			<pubDate>Tue, 25 Mar 2014 22:37:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/52951/#p52951</guid>
		</item>
		<item>
			<title><![CDATA[Re: extruder crashes on print end with with repetier]]></title>
			<link>https://www.soliforum.com/post/52950/#p52950</link>
			<description><![CDATA[<p>Repetier has its own End Code tab in the gcode window.&nbsp; Maybe it ended up in there somehow.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Tue, 25 Mar 2014 22:35:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/52950/#p52950</guid>
		</item>
		<item>
			<title><![CDATA[extruder crashes on print end with with repetier]]></title>
			<link>https://www.soliforum.com/post/52948/#p52948</link>
			<description><![CDATA[<p>I have a new install of repetier host on windows, and at the end of a calibration print, sliced with slic3r in repetier, the extruder does<br />G1 X-9 Y0 F4800</p><p>Crashes briefly, and then the motors turn off.&nbsp; The end of the print, including that command, are pasted below.</p><p>I can&#039;t find this command in my start or end code (which I have not modified), and I think my printer settings are either untouched, or I made sure they are copied from the solidoodle website recommendations.&nbsp; I just don&#039;t know where that command came from!</p><div class="codebox"><pre><code>...
19:35:51.390 : N4934 G1 X67.211 Y77.117 E5.46445 *126
19:35:51.437 : ok
19:35:51.437 : N4935 G1 E2.96445 F9000 *31
19:35:51.437 : N4936 G92 E0 *95
19:35:51.437 : N4937 M107 *60
19:35:51.515 : ok
19:35:51.515 : N4938 G28 X159 Y150 *13
19:35:51.562 : ok
19:35:51.562 : ok
19:35:51.562 : N4939 G91 *6
19:35:51.562 : N4940 G1 Z50 F50 *45
19:35:57.203 : ok
19:35:57.203 : ok
19:35:57.203 : ok
19:35:57.203 : Printjob finished at 3/24/2014 7:35 PM
19:35:57.203 : Printing Time:2m:47s
19:35:57.203 : Lines Send:1579
19:35:57.234 : N4942 G90 *11
19:35:57.234 : N4943 M104 T0 S0 *59
19:35:57.234 : ok T:195.9 /195.0 B:74.1 /75.0 @:86
19:35:57.234 : ok
19:35:57.234 : N4944 G1 X-9 Y0 F4800 *122
19:35:57.234 : N4945 M84 *3
19:35:57.234 : ok
...</code></pre></div><p>Is this a common problem?&nbsp; What is the solution?</p>]]></description>