<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Walls/lines slightly wavy]]></title>
		<link>https://www.soliforum.com/topic/5734/wallslines-slightly-wavy/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5734/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Walls/lines slightly wavy.]]></description>
		<lastBuildDate>Mon, 03 Mar 2014 06:17:03 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Walls/lines slightly wavy]]></title>
			<link>https://www.soliforum.com/post/51323/#p51323</link>
			<description><![CDATA[<p>Wouldn&#039;t z-wobbling only cause problems between multiple layers? &quot;wave.jpg&quot; is a single layer and it has this slightly wavy pattern which I&#039;m assuming is the cause of my problems.<br />Thanks.</p>]]></description>
			<author><![CDATA[null@example.com (maryla)]]></author>
			<pubDate>Mon, 03 Mar 2014 06:17:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/51323/#p51323</guid>
		</item>
		<item>
			<title><![CDATA[Re: Walls/lines slightly wavy]]></title>
			<link>https://www.soliforum.com/post/51292/#p51292</link>
			<description><![CDATA[<p>Looks like z-wobble.... it will show up worse if you are overextruding.</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Sun, 02 Mar 2014 19:44:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/51292/#p51292</guid>
		</item>
		<item>
			<title><![CDATA[Walls/lines slightly wavy]]></title>
			<link>https://www.soliforum.com/post/51288/#p51288</link>
			<description><![CDATA[<p>Hi, I have the original Solidoodle, and recently I&#039;ve been experiencing problems with my prints.<br />Walls are not as straight as they used to be. It looks to me like it&#039;s not printing straight lines any more. See pictures.</p><p>The red cube is an old print and is pretty good.<br />The white cube is from today and is not as good.<br />The third pictures is a test where you can see some waving on the border.</p><p>Any idea what&#039;s causing this and how I can fix it?<br />I&#039;ve had issues with banding in the past but I think this is different.<br />Thanks for you help!</p>]]></description>