		<title><![CDATA[SoliForum - 3D Printing Community — What exactly comes in the Electronics only kit for the filawinder?]]></title>
		<link>https://www.soliforum.com/topic/5575/what-exactly-comes-in-the-electronics-only-kit-for-the-filawinder/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5575/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in What exactly comes in the Electronics only kit for the filawinder?.]]></description>
		<lastBuildDate>Sat, 15 Feb 2014 23:51:15 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49854/#p49854</link>
			<description><![CDATA[<p>Curious what material you are cutting your enclosures out of? Is that just a 1/4&quot; melamine?</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 23:51:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49854/#p49854</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49852/#p49852</link>
			<description><![CDATA[<p>Good call Ian. I did sort of throw that together.&nbsp; </p><p>Also 3 hours for a nice looking store is great.&nbsp; I have spent a lot more time on my open cart version and I am not sure how much more it got me other then I am much better at web development. </p><p>Also I am very excited that the enclosure is open source.&nbsp; It&#039;s going to look ver nice in my shop:)</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 23:47:56 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49852/#p49852</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49849/#p49849</link>
			<description><![CDATA[<p>The change is fine, but I would go with-</p><p>* - Electronics Only kit includes these items.</p><p>I wouldn&#039;t want people to think that those only come with the electronics kit and they would need to buy both for a fully functioning winder.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Sat, 15 Feb 2014 23:10:51 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49849/#p49849</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49847/#p49847</link>
			<description><![CDATA[<div class="quotebox"><cite>pastprimitive wrote:</cite><blockquote><p>I love your product! I actually had an approval for 40 hours of donated work by Battelle National Laboratories to develop the exact same product for my small business.&nbsp; The engineer they assigned to me dragged his feet for 6 months.&nbsp; I stumbled across your kickstarted page, and knew you had hit the product right on the head. If you saw my initial conceptual sketches... They are identical. I am just super excited it got to market, and you seem to be running an amazing operation. Kudos to you!</p><p>Hopefully you can forgive me for my nit pickyness. To make up for it I ordered one. Just kidding, I would have ordered one even if you were a jerk. I LOVE THIS PRODUCT! <img src="https://www.soliforum.com/img/smilies/big_smile.png" width="15" height="15" alt="big_smile" /></p><p>You wouldn&#039;t by chance be willing to share a DXF file for the enclosure so I can cut it out for my soon to come filawinder on my home CNC router I have:) Understand completely if you don&#039;t want to;)</p></blockquote></div><br /><p>Nice! Thank for the kind words. I&#039;d love to be able to get back to R&amp;D soon.</p><p>Enclosure is open source, here&#039;s the DXFs:</p><p><a href="https://www.thingiverse.com/thing:145960">https://www.thingiverse.com/thing:145960</a></p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:55:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49847/#p49847</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49846/#p49846</link>
			<description><![CDATA[<div class="quotebox"><cite>pastprimitive wrote:</cite><blockquote><p>All right so I took a look so I could actually be helpful and not just a pain.&nbsp; I run an online store as well so I am a bit familiar with dealing with unruly customers such as myself;) </p><p>Is that the Opencart engine you are running yours on?&nbsp; Or something else?</p><p>I think having multiple places is helpful, customers can be daft, we all can be daft.&nbsp; I like one at the bottom, bt because links aren&#039;t underlined (which is fine in my opinion) it would be helpful to include them in addition up at the top.</p><div class="quotebox"><blockquote><p>...filament follows a steady, unchanging path from extruder to winder making it easy to produce professional quality filament for hours without worry.</p><p><strong>Kit Includes:</strong><br /></p><ul><li><p>Motor</p></li><li><p>Laser Cut Chasis</p></li><li><p>mounting hardware</p></li><li><p>PTFE Tubing</p></li><li><p>Sensing Laser</p></li><li><p>Switches &amp; Potentiometer</p></li><li><p>Control Board<span style="color: red">*</span></p></li><li><p>Sensor Board<span style="color: red">*</span></p></li><li><p>Jumper Wires<span style="color: red">*</span></p></li></ul><p><span style="color: red">*</span> - Electronics only kit.</p><p>Closed Loop Control -&nbsp; A sensor detects the position of the filament and adjusts the speed of the winder so it is never too fast or too slow.&nbsp; No...</p></blockquote></div></blockquote></div><p>It runs on Shopify. I took a total of like 3 hours setting it (the whole store) up, I&#039;m sure it could be revamped.</p><p>If Ian approved the changes (its his product), I&#039;m happy to make them!</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:53:26 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49846/#p49846</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49845/#p49845</link>
			<description><![CDATA[<p>And here&#039;s a link to my store if you want to make fun;) Running Opencart. You&#039;re store looks great BTW.</p><p><a href="http://pastprimitive.com/index.php?route=product/product&amp;product_id=81">http://pastprimitive.com/index.php?rout … duct_id=81</a></p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:23:28 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49845/#p49845</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49844/#p49844</link>
			<description><![CDATA[<p>I would have bought the enclosure, but after a new iMac, new laser cutter, and filawinder.... my tax return is about burned out.</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:21:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49844/#p49844</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49843/#p49843</link>
			<description><![CDATA[<p>I love your product! I actually had an approval for 40 hours of donated work by Battelle National Laboratories to develop the exact same product for my small business.&nbsp; The engineer they assigned to me dragged his feet for 6 months.&nbsp; I stumbled across your kickstarted page, and knew you had hit the product right on the head. If you saw my initial conceptual sketches... They are identical. I am just super excited it got to market, and you seem to be running an amazing operation. Kudos to you!</p><p>Hopefully you can forgive me for my nit pickyness. To make up for it I ordered one. Just kidding, I would have ordered one even if you were a jerk. I LOVE THIS PRODUCT! <img src="https://www.soliforum.com/img/smilies/big_smile.png" width="15" height="15" alt="big_smile" /></p><p>You wouldn&#039;t by chance be willing to share a DXF file for the enclosure so I can cut it out for my soon to come filawinder on my home CNC router I have:) Understand completely if you don&#039;t want to;)</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:19:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49843/#p49843</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49841/#p49841</link>
			<description><![CDATA[<p>All right so I took a look so I could actually be helpful and not just a pain.&nbsp; I run an online store as well so I am a bit familiar with dealing with unruly customers such as myself;) </p><p>Is that the Opencart engine you are running yours on?&nbsp; Or something else?</p><p>I think having multiple places is helpful, customers can be daft, we all can be daft.&nbsp; I like one at the bottom, bt because links aren&#039;t underlined (which is fine in my opinion) it would be helpful to include them in addition up at the top.</p><div class="quotebox"><blockquote><p>...filament follows a steady, unchanging path from extruder to winder making it easy to produce professional quality filament for hours without worry.</p><p><strong>Kit Includes:</strong><br /></p><ul><li><p>Motor</p></li><li><p>Laser Cut Chasis</p></li><li><p>mounting hardware</p></li><li><p>PTFE Tubing</p></li><li><p>Sensing Laser</p></li><li><p>Switches &amp; Potentiometer</p></li><li><p>Control Board<span style="color: red">*</span></p></li><li><p>Sensor Board<span style="color: red">*</span></p></li><li><p>Jumper Wires<span style="color: red">*</span></p></li></ul><p><span style="color: red">*</span> - Electronics only kit.</p><p>Closed Loop Control -&nbsp; A sensor detects the position of the filament and adjusts the speed of the winder so it is never too fast or too slow.&nbsp; No...</p></blockquote></div>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 22:15:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49841/#p49841</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49838/#p49838</link>
			<description><![CDATA[<p>I&#039;m happy to take suggestions on where to put the link to it! I tried to keep things organized by putting all the links at the bottom instead of haphazardly all over the place.</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 15 Feb 2014 21:31:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49838/#p49838</guid>
		</item>
		<item>
			<title><![CDATA[Re: What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49834/#p49834</link>
			<description><![CDATA[<p>And, I&#039;m a dipstick, I found the link to the included parts.&nbsp; Perhaps a bit more visible, or in the product description itself, was a bit hard to find.</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 21:05:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49834/#p49834</guid>
		</item>
		<item>
			<title><![CDATA[What exactly comes in the Electronics only kit for the filawinder?]]></title>
			<link>https://www.soliforum.com/post/49833/#p49833</link>
			<description><![CDATA[<p>Can&#039;t seem to track down what you&#039;re getting with the electronics only kit for the filawinder. Is it just the main pcb board and sensor board? Or do you get the laser pointer as well?&nbsp; A detailed list of what comes with the kit on the site would be nice, or point me to it if I have missed it.&nbsp; I am really itching to pick one up;)</p>]]></description>
			<author><![CDATA[null@example.com (pastprimitive)]]></author>
			<pubDate>Sat, 15 Feb 2014 21:03:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/49833/#p49833</guid>
		</item>