<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Filastruder / FilaWinder black segment and stretch marks]]></title>
		<link>https://www.soliforum.com/topic/5404/filastruder-filawinder-black-segment-and-stretch-marks/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5404/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Filastruder / FilaWinder black segment and stretch marks.]]></description>
		<lastBuildDate>Sun, 02 Feb 2014 20:42:37 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48478/#p48478</link>
			<description><![CDATA[<p>Thanks CraigRK.</p><p>Ian, I did have PLA in there at one point in the past when I first attempted to extrude PLA without dehydrating it and failed miserably. That was a couple weeks ago. I did take apart all the parts the pellets/filament pass through and cleaned them thoroughly, but maybe there were some pieces left over. However, this IS the first time I try to extrude at this temperature (192.5c). The last 2lb spool I made was extruded at 185c. So perhaps the temperature change did have something to do with it. I&#039;ll try your suggestion of lowering the temperature temporarily to purge out the PLA and then I think I&#039;ll stick to 185c for my next spool, but without a fan.</p>]]></description>
			<author><![CDATA[null@example.com (malek1979m)]]></author>
			<pubDate>Sun, 02 Feb 2014 20:42:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48478/#p48478</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48475/#p48475</link>
			<description><![CDATA[<div class="quotebox"><cite>malek1979m wrote:</cite><blockquote><p>But is this actually natural filament? I thought natural pellets/filament would have been transparent, yet my prints, even if they are single walled, are far from transparent.</p></blockquote></div><p>The first ABS filament I bought (and am still using) is natural, and it definitely is NOT transparent.&nbsp; The same for the ABS pellets I have.</p><div class="quotebox"><cite>malek1979m wrote:</cite><blockquote><p> I don&#039;t think I&#039;ve seen white colourant on any site...</p></blockquote></div><p>I think most don&#039;t stock it as they assume people are happy to settle for the offwhite that Natural gives.</p><p>I stock white masterbatch (See Tim&#039;s &quot;Polymer Suppliers&quot; sticky) as I thought it would be useful if people wanted to the make things like pinks, etc.&nbsp; In other words, white is very much available and neededif you want to make white filament.</p>]]></description>
			<author><![CDATA[null@example.com (CraigRK)]]></author>
			<pubDate>Sun, 02 Feb 2014 19:30:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48475/#p48475</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48473/#p48473</link>
			<description><![CDATA[<p>Were you running PLA before switching to ABS?&nbsp; Looks like not all of the PLA was purged.&nbsp; When I switched from ABS to PLA once I found that I kept getting bits of ABS in the PLA, which was easy to see since the PLA was clear.&nbsp; I found that if it ran hotter, the PLA seemed to slide past the leftover ABS, but if it was cooler the increased viscosity would start to drag the ABS out.&nbsp; </p><p>It may be true the other way around.&nbsp; If you need to purge PLA try running the ABS at a lower temp for awhile so the extra friction can scour the sides of the barrel.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Sun, 02 Feb 2014 18:53:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48473/#p48473</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48472/#p48472</link>
			<description><![CDATA[<p>That makes sense. I&#039;ll try that.<br />And thank you in advance for the PTFE, I appreciate it. But will a longer piece make a difference to the final product?</p><p>I looked at my nozzle tip and saw this:</p><p><span class="postimg"><img src="https://dl.dropboxusercontent.com/u/60513393/IMG_20140202_131855.jpg" alt="https://dl.dropboxusercontent.com/u/60513393/IMG_20140202_131855.jpg" /></span></p><p>Talk about ew! Why is this happening? I have a feeling it has something to do with the gray-ish filament.</p>]]></description>
			<author><![CDATA[null@example.com (malek1979m)]]></author>
			<pubDate>Sun, 02 Feb 2014 18:24:36 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48472/#p48472</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48469/#p48469</link>
			<description><![CDATA[<p>I&#039;ve seen natural ABS come out pretty gray when it gets overheated around +200C.&nbsp; &nbsp;Maybe at 192 some of it got hot enough at some point to catch just a shade of it.&nbsp; That&#039;s nozzle temperature, I don&#039;t know how hot it gets in the melt zone to cause that.&nbsp; &nbsp;You might try sliding the heater band a little closer to the nozzle so it doesn&#039;t have to get as hot to give you 192 at the opening.</p><p>I have another batch of the 6mm PTFE on the way, I&#039;ll send you a longer length of it when it comes in.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Sun, 02 Feb 2014 17:38:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48469/#p48469</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48466/#p48466</link>
			<description><![CDATA[<p>Natural ABS is most definitely not transparent. Here&#039;s some white colorant.</p><p><a href="http://www.indhobbies.com/Masterbatch_Colorant.html">http://www.indhobbies.com/Masterbatch_Colorant.html</a></p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 02 Feb 2014 17:06:00 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48466/#p48466</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48463/#p48463</link>
			<description><![CDATA[<p>But is this actually natural filament? I thought natural pellets/filament would have been transparent, yet my prints, even if they are single walled, are far from transparent. I don&#039;t think I&#039;ve seen white colourant on any site...<br />And using a larger ID spool would not work because the stretch marks are created right after coming out of the PTFE tube, and it&#039;s as big a diameter as it gets. Hm... I wonder what would happen if I used another PTFE tube with a much larger diameter... Why is it so small anyways? It&#039;s a lot smaller than the 1.75mm PTFE that comes with the kit.</p>]]></description>
			<author><![CDATA[null@example.com (malek1979m)]]></author>
			<pubDate>Sun, 02 Feb 2014 16:52:43 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48463/#p48463</guid>
		</item>
		<item>
			<title><![CDATA[Re: Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48462/#p48462</link>
			<description><![CDATA[<p>Not sure what would have caused the dark segment, but since you aren&#039;t putting any colorant in it wouldn&#039;t take much to color it. If you want truly white, you need to add white colorant. Natural ABS does not contain colorant.</p><p>Stretch marks shouldn&#039;t be a problem after printing. I&#039;ve never seen that before with 1.75mm filament, can you use a larger ID spool?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sun, 02 Feb 2014 16:45:26 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48462/#p48462</guid>
		</item>
		<item>
			<title><![CDATA[Filastruder / FilaWinder black segment and stretch marks]]></title>
			<link>https://www.soliforum.com/post/48460/#p48460</link>
			<description><![CDATA[<p>I&#039;m filastruding and filawinding nicely and consistently now, but I did notice a couple things that were troubling me. One thing is that about half way through filastruding and filawinding 2 lbs of white ABS, I noticed a segment (several feet) of filament was actually not white, like it was very dark, as if burned (see picture, right in the middle of the spool, although it&#039;s hard to see, but it&#039;s that area that is a bit darker. It may look like a shadow, and a little bit of it is, but it&#039;s mostly just dark). Let me tell you that I have not yet put a shred of any colourant in the filastruder. I have only used white so far. Any idea what could cause that? I&#039;m extruding 3mm ABS filament (actual: 2.85mm) at 192.5 c, vertically.</p><p>The other issue I&#039;m having is the apparent stretch marks on the filament after it is wound (right after it comes out of the PTFE tube). This probably doesn&#039;t happen with 1.75mm filament, but 3mm is very stiff and as soon as it starts bending a little, you can see stretch marks on the entire thing. How come filament you purchase doesn&#039;t look like that? I have a feeling that one way to fix this would be to slightly heat up the filament immediately prior to spooling it to a specific temperature that won&#039;t change the filament consistency but will be just enough to soften it for easy spooling. Do you think this would work? I had this crazy idea to try to point a halogen light (see picture) at the spool just far enough to soften the filament. I&#039;ve actually been using a halogen light just like this one in certain cases to heat up ABS/PLA parts after printing them so I can mold them a little if they don&#039;t come out perfect. Like if a part warps, I&#039;ve actually been able to unwarp it using this method. Any ideas?</p><p><span class="postimg"><img src="https://dl.dropboxusercontent.com/u/60513393/IMG_20140202_114530.jpg" alt="https://dl.dropboxusercontent.com/u/60513393/IMG_20140202_114530.jpg" /></span><br /><span class="postimg"><img src="https://dl.dropboxusercontent.com/u/60513393/halogen%20light.jpg" alt="https://dl.dropboxusercontent.com/u/60513393/halogen%20light.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (malek1979m)]]></author>
			<pubDate>Sun, 02 Feb 2014 16:42:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48460/#p48460</guid>