<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Switching between ABS and PLA and vs Versa]]></title>
		<link>https://www.soliforum.com/topic/5372/switching-between-abs-and-pla-and-vs-versa/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5372/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Switching between ABS and PLA and vs Versa.]]></description>
		<lastBuildDate>Sat, 01 Feb 2014 18:49:55 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Switching between ABS and PLA and vs Versa]]></title>
			<link>https://www.soliforum.com/post/48391/#p48391</link>
			<description><![CDATA[<p>Thanks, your post I think will help a lot.&nbsp; I had cleaned out everything and reassembled, plugged up again when using transparent blue pla.&nbsp; Again at 175c.&nbsp; It didn&#039;t occur that I should use a higher temperature, which, when I get brave enough to try again I will do.&nbsp; I had to rip apart the head again and because the last rebuild leaked pla from the heatbreak, I used some Teflon tape to seal it, so far so good, but only printing with ABS right now.</p><p>Thanks again<br />&nbsp; Andrew</p>]]></description>
			<author><![CDATA[null@example.com (doppler)]]></author>
			<pubDate>Sat, 01 Feb 2014 18:49:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48391/#p48391</guid>
		</item>
		<item>
			<title><![CDATA[Re: Switching between ABS and PLA and vs Versa]]></title>
			<link>https://www.soliforum.com/post/48310/#p48310</link>
			<description><![CDATA[<p>I mostly do the same thing: <br />1. Heat to ABS temp.<br />2. Extract remaining ABS filament.<br />3. Switch to PLA.<br />4. Keep at ABS temp and extrude at least 300 mm of the new PLA (more if the PLA is a much lighter color than the ABS) - I set the speed to 200 for this, thinking that the PLA runs fast enough that it won&#039;t clog up.<br />5. Lower the temp to PLA and try to start the print job without sitting too long.</p><p>I&#039;ve had some PLA that needs to print around 180, and I got one spool of translucent purple that seemed to need 190 (so it was basically running at ABS temp).&nbsp; &nbsp;Right now, I have a yellow ABS that needs 210.</p>]]></description>
			<author><![CDATA[null@example.com (fredhag)]]></author>
			<pubDate>Fri, 31 Jan 2014 07:20:40 +0000</pubDate>
			<guid>https://www.soliforum.com/post/48310/#p48310</guid>
		</item>
		<item>
			<title><![CDATA[Switching between ABS and PLA and vs Versa]]></title>
			<link>https://www.soliforum.com/post/48284/#p48284</link>
			<description><![CDATA[<p>Yesterday I got my first rolls of PLA (Blue).&nbsp; I removed my Orange ABS from the printer, put the blue in, heated it to ABS temp and extruded, clearing as much of the ABS as I could, i know there can be quiet a bit hiding in the extruder.&nbsp; &nbsp;</p><p>Lowered the temperature to PLA (175c).&nbsp; Well I started printing an object, it was doing fairly well, for being uncalibrated for the new filament, I went a way for a bit and came back to find the printer not extruding for many layers.&nbsp; clogged.</p><p>I bumped up the heat to ABS levels to try and clear it, nope.&nbsp; Took it all apart, used a small torch to melt out all the crud, Brown, Orange + Blue goo.... </p><p>Now, I think I didn&#039;t do something right, how are you supposed to clear the ABS?&nbsp; Is there a procedure that prevents the above from happening?</p><p>Thanks<br />&nbsp; Andrew</p>]]></description>