<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Crazy mid air rafts from KISSlicer gcode]]></title>
		<link>https://www.soliforum.com/topic/519/crazy-mid-air-rafts-from-kisslicer-gcode/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/519/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Crazy mid air rafts from KISSlicer gcode.]]></description>
		<lastBuildDate>Thu, 15 Nov 2012 23:56:49 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4773/#p4773</link>
			<description><![CDATA[<p>The free version of Netfabb has less capability than the expensive Pro version.&nbsp; However I think the cloud service uses the Pro version, or something close.&nbsp; I don&#039;t think the cloud version will fix intersections, but it seems to have a few more tricks.&nbsp; I&#039;ve also had luck running difficult models through the cloud a couple of times, if the first upload didn&#039;t seem to fix it.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Thu, 15 Nov 2012 23:56:49 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4773/#p4773</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4772/#p4772</link>
			<description><![CDATA[<p>Ian,</p><p>I think I wasn&#039;t getting the model truly maniform in the desktop version of netfabb.&nbsp; I just put one of the same models I was having problems with through the cloud version and the stl looks fine in Kisslicer.</p>]]></description>
			<author><![CDATA[null@example.com (JustSomeGuyTN)]]></author>
			<pubDate>Thu, 15 Nov 2012 23:53:27 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4772/#p4772</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4506/#p4506</link>
			<description><![CDATA[<p>I will try when I&#039;m back home.&nbsp; I will probably have to host it off my website because it&#039;s a big file.</p>]]></description>
			<author><![CDATA[null@example.com (JustSomeGuyTN)]]></author>
			<pubDate>Tue, 13 Nov 2012 14:12:03 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4506/#p4506</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4505/#p4505</link>
			<description><![CDATA[<p>Can you post the STL?&nbsp; KS has been pretty solid for me where support is concerned.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Tue, 13 Nov 2012 13:42:42 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4505/#p4505</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4504/#p4504</link>
			<description><![CDATA[<p>Ian, </p><p>I had actually already downloaded netfabb and run it through the repair.&nbsp; Maybe I didn&#039;t pick the right options on it or something.</p>]]></description>
			<author><![CDATA[null@example.com (JustSomeGuyTN)]]></author>
			<pubDate>Tue, 13 Nov 2012 11:54:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4504/#p4504</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4486/#p4486</link>
			<description><![CDATA[<p>+1 for Ian&#039;s comment.</p><p>I find it will find (and fix) just about anything without messing up the model.&nbsp; Also- you don&#039;t have to wait for cloud processing.&nbsp; Your PC will do it in seconds.</p><p>Cheers</p>]]></description>
			<author><![CDATA[null@example.com (WhiteStar01)]]></author>
			<pubDate>Tue, 13 Nov 2012 01:48:52 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4486/#p4486</guid>
		</item>
		<item>
			<title><![CDATA[Re: Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4484/#p4484</link>
			<description><![CDATA[<p>It&#039;s possible that the STL has some issues that KS doesn&#039;t know how to deal with.&nbsp; Download NetFabb Studio Basic (free) <a href="http://www.netfabb.com/download.php">http://www.netfabb.com/download.php</a> and see if it gives you alerts about anything.</p>]]></description>
			<author><![CDATA[null@example.com (IanJohnson)]]></author>
			<pubDate>Tue, 13 Nov 2012 01:39:06 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4484/#p4484</guid>
		</item>
		<item>
			<title><![CDATA[Crazy mid air rafts from KISSlicer gcode]]></title>
			<link>https://www.soliforum.com/post/4483/#p4483</link>
			<description><![CDATA[<p>Can anyone explain why this happens and help me fix the issue?&nbsp; I&#039;m trying to generate some gcode in KISSlicer of a female super hero figure I made.&nbsp; But at certain points in the model it generates these crazy mid air rafts that aren&#039;t supporting anything and have no support themselves.&nbsp; They connect to the main model but all they will do is causing huge blobs on the sides of the model.&nbsp; I&#039;ve included a screen shot of what I&#039;m talking about.&nbsp; Also I am following the settings that Ian put out a while back for KISSlicer.</p>]]></description>
			<author><![CDATA[null@example.com (JustSomeGuyTN)]]></author>
			<pubDate>Tue, 13 Nov 2012 01:15:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/4483/#p4483</guid>
		</item>