<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — SD4 or Fusematic]]></title>
		<link>https://www.soliforum.com/topic/5082/sd4-or-fusematic/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/5082/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in SD4 or Fusematic.]]></description>
		<lastBuildDate>Mon, 06 Jan 2014 06:04:07 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: SD4 or Fusematic]]></title>
			<link>https://www.soliforum.com/post/45917/#p45917</link>
			<description><![CDATA[<p>It&#039;s my first printer.&nbsp; I&#039;m just looking at printing random things for fun or usefulness around the house.&nbsp; Nothing specific.&nbsp; Thanks for explaining both.&nbsp; </p><p>I&#039;m in Korea so my concern is getting parts in the future.&nbsp; It looked like the FM would be easier to upgrade.&nbsp; Seeing all the complaints about the lack of revisions that could have been made from the SD3 to the SD4 I guess scares me a bit.&nbsp; </p><p>They know of these issues but decided to not make any fixes.&nbsp; Which would you consider?&nbsp; Which do you have?</p>]]></description>
			<author><![CDATA[null@example.com (qtoppa)]]></author>
			<pubDate>Mon, 06 Jan 2014 06:04:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/45917/#p45917</guid>
		</item>
		<item>
			<title><![CDATA[Re: SD4 or Fusematic]]></title>
			<link>https://www.soliforum.com/post/45913/#p45913</link>
			<description><![CDATA[<p>Two different printers there... but the tech on both is pretty standard.</p><p>SD = direct extruder FM = Bowden extruder<br />SD = XY printhead FM = Mendel style sliding bed<br />electronics... about the same</p><p>It all depends on your needs/wants the bowden setup can speed things up quite a bit but needs to be really tuned to get good results when doing so... what are you looking to print and why?</p><p>Sounds like the FM is easy enough to put together even for newbies...</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Mon, 06 Jan 2014 05:45:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/45913/#p45913</guid>
		</item>
		<item>
			<title><![CDATA[SD4 or Fusematic]]></title>
			<link>https://www.soliforum.com/post/45891/#p45891</link>
			<description><![CDATA[<p>I&#039;m a new to the world of 3d printing.&nbsp; I&#039;ve been doing as much research as possible and have come down to these 2 3d printers.</p><p>SD4($1000) is enclosed and seems to have a great support forum but technology seems to be a bit outdated.</p><p>Fusematic ($850) has great technology (I think?) but is not enclosed.</p><p>Price point is pretty similar.</p><p>Which one would you go for and why?&nbsp; I heard the Fusematic extruder can be difficult but why? Thanks for your help in advance</p>]]></description>
			<author><![CDATA[null@example.com (qtoppa)]]></author>
			<pubDate>Mon, 06 Jan 2014 01:44:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/45891/#p45891</guid>
		</item>