<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Glass Plate --> Super glue --> painters tape -->platform]]></title>
		<link>https://www.soliforum.com/topic/4713/glass-plate-super-glue-painters-tape-platform/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/4713/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Glass Plate --> Super glue --> painters tape -->platform.]]></description>
		<lastBuildDate>Tue, 03 Dec 2013 16:24:29 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/43141/#p43141</link>
			<description><![CDATA[<p>It seems as though a lot of people have missed it.&nbsp; Every time I read a thread about glass clips or the like I try to toss it out there.&nbsp; It makes things so much easier.&nbsp; You may need to use a razor blade to gently pry (less pry and more slip in between) the glass from the bed the first time you have to remove it.&nbsp; After that it just pulls off by grabbing the print itself.&nbsp; Even if it doesn&#039;t seem like it isn&#039;t sticking that well (it will once it heats up) I have never had my glass move during a print.</p>]]></description>
			<author><![CDATA[null@example.com (wardjr)]]></author>
			<pubDate>Tue, 03 Dec 2013 16:24:29 +0000</pubDate>
			<guid>https://www.soliforum.com/post/43141/#p43141</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/43140/#p43140</link>
			<description><![CDATA[<div class="quotebox"><cite>wardjr wrote:</cite><blockquote><p>(copied from glass bed hacks and mods)<br />I&#039;ve said it before and I will say it again.&nbsp; Leave the Kapton on the platform then spray the underside of your glass with the same hairspray you put on the top side.&nbsp; Put the glass on your platform and heat it up.&nbsp; No clips, perfectly level glass and it sticks well enough to not move and is still easy enough to remove.&nbsp; And no I don&#039;t have to respray every time I remove it.<br />I run my bed at 108 and everything seems happy.</p></blockquote></div><p>Not sure how I missed this but this is an awesome idea!&nbsp; Can&#039;t wait to try it out</p>]]></description>
			<author><![CDATA[null@example.com (jason_)]]></author>
			<pubDate>Tue, 03 Dec 2013 16:17:23 +0000</pubDate>
			<guid>https://www.soliforum.com/post/43140/#p43140</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/43139/#p43139</link>
			<description><![CDATA[<p>(copied from glass bed hacks and mods)<br />I&#039;ve said it before and I will say it again.&nbsp; Leave the Kapton on the platform then spray the underside of your glass with the same hairspray you put on the top side.&nbsp; Put the glass on your platform and heat it up.&nbsp; No clips, perfectly level glass and it sticks well enough to not move and is still easy enough to remove.&nbsp; And no I don&#039;t have to respray every time I remove it.<br />I run my bed at 108 and everything seems happy.</p>]]></description>
			<author><![CDATA[null@example.com (wardjr)]]></author>
			<pubDate>Tue, 03 Dec 2013 16:14:16 +0000</pubDate>
			<guid>https://www.soliforum.com/post/43139/#p43139</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/42971/#p42971</link>
			<description><![CDATA[<p>Thanks, I&#039;ll keep that in mind!&nbsp; </p><p>Perhaps I&#039;ll do some tests, but now I don&#039;t want to remove the glass if this is just dumb luck!</p><p>I will look into high heat glue for future use!</p>]]></description>
			<author><![CDATA[null@example.com (dpotthast)]]></author>
			<pubDate>Sun, 01 Dec 2013 10:48:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42971/#p42971</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/42970/#p42970</link>
			<description><![CDATA[<p>Its not the glass - its the chemistry of Cyanoacrylate. In standard form it has a service temp of -50°C to 80°C..&nbsp; That means, at temps above 80°C it is outside its bond specs.&nbsp; Ethyl-2 Cyanoacrylate is what you call &#039;super glue&#039;.... </p><p>Checking the MSDS for Duro, it is bog stock Ethyl-2&nbsp; Cyanoacrylate... <a href="http://hpd.nlm.nih.gov/cgi-bin/household/brands?tbl=brands&amp;id=13010011">http://hpd.nlm.nih.gov/cgi-bin/househol … d=13010011</a></p><p>There is newer formulas that include additional additives to boost that service temp to 125°C (usually) - but it is not what Duro is made of according to its MSDS... </p><p>So if its staying bonded at temps &gt;80°C - don&#039;t loose that tube of glue - its super super-glue <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p><p>EDIT: <a href="http://en.wikipedia.org/wiki/Ethyl_cyanoacrylate">http://en.wikipedia.org/wiki/Ethyl_cyanoacrylate</a> &lt;- lists the service temp as -54°C to 82°C.. so I wasn&#039;t far off <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p><p>Anyway - despite your personal success - this is why its not recommended by the vast majority of people - It works for a while, but it will fail - probably with more tangential forces yours would have most likely failed by now already too - A good solid knock to the glass when its warm for example....</p>]]></description>
			<author><![CDATA[null@example.com (adrian)]]></author>
			<pubDate>Sun, 01 Dec 2013 10:28:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42970/#p42970</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/42969/#p42969</link>
			<description><![CDATA[<p>hmm.. I have not had any issues heating bed to 100C&nbsp; .&nbsp; My superglue is nothing special, picked it up at Target...&nbsp; &quot;Duro&quot; brand...</p><p>edit*<br />my glass does have a slight texture on the base... perhaps that is the reason for better stick?</p>]]></description>
			<author><![CDATA[null@example.com (dpotthast)]]></author>
			<pubDate>Sun, 01 Dec 2013 10:19:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42969/#p42969</guid>
		</item>
		<item>
			<title><![CDATA[Re: Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/42966/#p42966</link>
			<description><![CDATA[<div class="quotebox"><cite>dpotthast wrote:</cite><blockquote><p>Simple way to attach glass bed <strong>without clips</strong>... hear me out...&nbsp; super glue!&nbsp; </p><p>1) lay down some painters tape on your bed in an x pattern, corners to corners<br />2) put <em>single</em> drops of super glue on the bottom of your glass, the four corners and the center<br />3) place your glass</p><p>if you have to take it off, peel the painters tape with it or, if you used little enough glue, the glass might just pop off the tape.</p><p>The main reason I did this was to keep my print area as large as possible without the chance of the extruder running over the clips, potentially damaging it, or getting caught.</p><p>I have been running strong with this method for over two months now, no ill effects...</p></blockquote></div><p>As per the other 2 threads you&#039;ve posted this into:</p><p>What temp you run the bed at, or what super glue specifically did you use ?<br />Unless its the specifically marked high temp stuff - then that is very unusual to last that long.. &#039;standard&#039; cyanoacrylate is only good to 80°C and will fail at that temp.... only the newer high-temp special stuff is rated higher..</p><p>But glad to hear its worked out ok so far! <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> - anyone else who has used superglue has had it fail after a period of time for the reasons I just outlined.</p>]]></description>
			<author><![CDATA[null@example.com (adrian)]]></author>
			<pubDate>Sun, 01 Dec 2013 09:46:47 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42966/#p42966</guid>
		</item>
		<item>
			<title><![CDATA[Glass Plate --> Super glue --> painters tape -->platform]]></title>
			<link>https://www.soliforum.com/post/42962/#p42962</link>
			<description><![CDATA[<p>(also posted in glass bed hacks and mods)</p><p>Simple way to attach glass bed <strong>without clips</strong>... hear me out...&nbsp; super glue!&nbsp; </p><p>1) lay down some painters tape on your bed in an x pattern, corners to corners<br />2) put <em>single</em> drops of super glue on the bottom of your glass, the four corners and the center<br />3) place your glass</p><p>if you have to take it off, peel the painters tape with it or, if you used little enough glue, the glass might just pop off the tape.</p><p>The main reason I did this was to keep my print area as large as possible without the chance of the extruder running over the clips, potentially damaging it, or getting caught.</p><p>I have been running strong with this method for over two months now, no ill effects...</p>]]></description>
			<author><![CDATA[null@example.com (dpotthast)]]></author>
			<pubDate>Sun, 01 Dec 2013 09:28:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42962/#p42962</guid>