<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Gaps and "Bobbles" in perimeters]]></title>
		<link>https://www.soliforum.com/topic/4698/gaps-and-bobbles-in-perimeters/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/4698/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Gaps and "Bobbles" in perimeters.]]></description>
		<lastBuildDate>Tue, 03 Dec 2013 14:35:22 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Gaps and "Bobbles" in perimeters]]></title>
			<link>https://www.soliforum.com/post/43130/#p43130</link>
			<description><![CDATA[<p>I will try that thanks (once I get the Hot End repaired/refitted)</p>]]></description>
			<author><![CDATA[null@example.com (markthorpe)]]></author>
			<pubDate>Tue, 03 Dec 2013 14:35:22 +0000</pubDate>
			<guid>https://www.soliforum.com/post/43130/#p43130</guid>
		</item>
		<item>
			<title><![CDATA[Re: Gaps and "Bobbles" in perimeters]]></title>
			<link>https://www.soliforum.com/post/42839/#p42839</link>
			<description><![CDATA[<p>You should experiment with your retraction and restart values as they affect the blobs you are seeing, I haven&#039;t used skeinforge for a long time so no idea?? but I think a couple of people here still use it... maybe they will offer up some tuning suggestions.</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Fri, 29 Nov 2013 19:19:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42839/#p42839</guid>
		</item>
		<item>
			<title><![CDATA[Gaps and "Bobbles" in perimeters]]></title>
			<link>https://www.soliforum.com/post/42823/#p42823</link>
			<description><![CDATA[<p>Hello all,<br />I seem to be getting the odd gap in the perimeter on an otherwise good print. There are also &quot;bobbles&quot; on the outside of the perimeter present all the way up the layers. These seem to coincide with where each layer begins the print.<br />Here&#039;s what I have so far:</p><p>Solidoodle 2 - enclosed<br />Material: ABS 1.75mm<br />Temp: 210 1st layer, 200 rest<br />Bed: 105 degrees Kapton<br />Software: Repetier/Skeinforge<br />Brand new hot end<br />Level Bed<br />Calibrated flow and dimension</p><p>Could it simply be that the ABS is sometimes not getting pulled through (maybe tension on the rollers) that can cause these gaps in seemingly random places ? Also - what about the bobbles of plastic at the starting point - anyone else get these ?<br />Video attached as a photo did not show problem in enough detail.</p><p>Cheers</p>]]></description>
			<author><![CDATA[null@example.com (markthorpe)]]></author>
			<pubDate>Fri, 29 Nov 2013 10:58:19 +0000</pubDate>
			<guid>https://www.soliforum.com/post/42823/#p42823</guid>