<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Best Glue]]></title>
		<link>https://www.soliforum.com/topic/4578/best-glue/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/4578/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Best Glue.]]></description>
		<lastBuildDate>Mon, 18 Nov 2013 22:20:24 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Best Glue]]></title>
			<link>https://www.soliforum.com/post/41917/#p41917</link>
			<description><![CDATA[<p>I use Acrylic Cement from Tap Plastics.&nbsp; The stuff is free flowing so it&#039;s easy to apply with a hypo to get a capilary action at the joints.&nbsp; Since it&#039;s like acetone only 10 times more concentrated, it bonds the plasctic parts together by melting the plastic surfaces together.&nbsp; The resulting weld is as strong as if the part was made as one piece.</p><p><a href="https://www.tapplastics.com/product/repair_products/plastic_adhesives/tap_acrylic_cement/130">https://www.tapplastics.com/product/rep … cement/130</a></p><p>Of course this only works with ABS.&nbsp; For PLA, I use either CA glue (cyanoacrylate/crazy glue) or epoxy if a I need a more reliable bond.</p>]]></description>
			<author><![CDATA[null@example.com (pirvan)]]></author>
			<pubDate>Mon, 18 Nov 2013 22:20:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/41917/#p41917</guid>
		</item>
		<item>
			<title><![CDATA[Re: Best Glue]]></title>
			<link>https://www.soliforum.com/post/41913/#p41913</link>
			<description><![CDATA[<p><a href="http://www.dickblick.com/products/plastruct-bondene-cement/">Plastruct Bondene</a> works incredibly well.&nbsp; From the link:</p><div class="quotebox"><blockquote><p>Bondene works by dissolving a thin layer of plastic material on each surface to be joined. Once the cement evaporates, a continuous solid weld is formed — one as strong as the surrounding plastic.</p></blockquote></div>]]></description>
			<author><![CDATA[null@example.com (Boz)]]></author>
			<pubDate>Mon, 18 Nov 2013 20:16:41 +0000</pubDate>
			<guid>https://www.soliforum.com/post/41913/#p41913</guid>
		</item>
		<item>
			<title><![CDATA[Best Glue]]></title>
			<link>https://www.soliforum.com/post/41912/#p41912</link>
			<description><![CDATA[<p>What&#039;s the best glue to hold Solidoodle objects together?&nbsp; Would Hot Stuff work or would that melt the plastic to much?</p>]]></description>
			<author><![CDATA[null@example.com (MartinFahrer)]]></author>
			<pubDate>Mon, 18 Nov 2013 20:11:25 +0000</pubDate>
			<guid>https://www.soliforum.com/post/41912/#p41912</guid>
		</item>
	</channel>
</rss>