<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Calibration and now problems]]></title>
		<link>https://www.soliforum.com/topic/4416/calibration-and-now-problems/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/4416/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Calibration and now problems.]]></description>
		<lastBuildDate>Mon, 04 Nov 2013 13:35:57 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Calibration and now problems]]></title>
			<link>https://www.soliforum.com/post/40672/#p40672</link>
			<description><![CDATA[<p>I did the 100 mm test and thats were i got my 25% off....but then i got busy and forgot that i hadnt done the cube test.&nbsp; Did the cube test this weekend and found my problem in doing that.&nbsp; All is pretty much right with it now.&nbsp; Thanks for the reply though!</p>]]></description>
			<author><![CDATA[null@example.com (chuddly)]]></author>
			<pubDate>Mon, 04 Nov 2013 13:35:57 +0000</pubDate>
			<guid>https://www.soliforum.com/post/40672/#p40672</guid>
		</item>
		<item>
			<title><![CDATA[Re: Calibration and now problems]]></title>
			<link>https://www.soliforum.com/post/40417/#p40417</link>
			<description><![CDATA[<p>Depends. What did you alter for extrusion and why? The proper way to calibrate extrusion is the 100mm test to get your steps/mm dialed in and save to your EEPROM through Repetier Host.</p><p>Then, you print a single wall cube and measure it using calipers to dial in your extrusion mutliplier in slicer. </p><p>So, if you have done exactly that, then we need to go into further adjustments.</p>]]></description>
			<author><![CDATA[null@example.com (Hazer)]]></author>
			<pubDate>Thu, 31 Oct 2013 20:33:58 +0000</pubDate>
			<guid>https://www.soliforum.com/post/40417/#p40417</guid>
		</item>
		<item>
			<title><![CDATA[Calibration and now problems]]></title>
			<link>https://www.soliforum.com/post/40408/#p40408</link>
			<description><![CDATA[<p>About a week ago i went through the calibrations for my extruder.&nbsp; I found that i was over extruding to the tune of about 25% (i could see it because the center infill was humped up higher than the outter walls and the nozzle would drag).&nbsp; So i got it set to the correct extrusion but now all of my models i print the outter walls dont make good contact with the infill or where 2 outter walls come close and just a slightly fatter than 1 bead it just puts dots everywhere inbetween.&nbsp; I dont have my settings handy or even a picture of it because im out of town but i can post them when i get home this weekend.&nbsp; Any thoughts though?&nbsp; It didnt do this before the calibration.&nbsp; But now my parts are much better on their size.</p>]]></description>