<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Heated Bed?]]></title>
		<link>https://www.soliforum.com/topic/288/heated-bed/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/288/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Heated Bed?.]]></description>
		<lastBuildDate>Thu, 11 Oct 2012 11:27:05 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Heated Bed?]]></title>
			<link>https://www.soliforum.com/post/2131/#p2131</link>
			<description><![CDATA[<p>Thank you both for the information.</p>]]></description>
			<author><![CDATA[null@example.com (bpaylor2002)]]></author>
			<pubDate>Thu, 11 Oct 2012 11:27:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/2131/#p2131</guid>
		</item>
		<item>
			<title><![CDATA[Re: Heated Bed?]]></title>
			<link>https://www.soliforum.com/post/2118/#p2118</link>
			<description><![CDATA[<p>if your bed is &quot;metal&quot; its a heated bed. <br />if its made of &quot;plastic&quot; its not.</p><p>heated bed is aluminium.<br />non heated bed is acrylic im pretty sure.</p><p>Correct me if im wrong someone.</p>]]></description>
			<author><![CDATA[null@example.com (macmub)]]></author>
			<pubDate>Thu, 11 Oct 2012 00:29:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/2118/#p2118</guid>
		</item>
		<item>
			<title><![CDATA[Re: Heated Bed?]]></title>
			<link>https://www.soliforum.com/post/2117/#p2117</link>
			<description><![CDATA[<p>the heated bed is a 100$ option that you choose when you buy your solidoodle 2.. if your bed is in plastic (acrylic)... it&#039;s not a heated bed..</p>]]></description>
			<author><![CDATA[null@example.com (ysb)]]></author>
			<pubDate>Thu, 11 Oct 2012 00:09:25 +0000</pubDate>
			<guid>https://www.soliforum.com/post/2117/#p2117</guid>
		</item>
		<item>
			<title><![CDATA[Heated Bed?]]></title>
			<link>https://www.soliforum.com/post/2116/#p2116</link>
			<description><![CDATA[<p>This might sound goofy, but I can&#039;t find a definitive answer.&nbsp; Does the Solidoodle II, come with a heated bed?&nbsp; If so, mine either isn&#039;t working or I need to buy a heated bed. If I need to buy a heated bed, any recommendations?&nbsp; H E L P !</p>]]></description>
			<author><![CDATA[null@example.com (bpaylor2002)]]></author>
			<pubDate>Wed, 10 Oct 2012 23:47:54 +0000</pubDate>
			<guid>https://www.soliforum.com/post/2116/#p2116</guid>
		</item>