<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Strange clog not normal]]></title>
		<link>https://www.soliforum.com/topic/2066/strange-clog-not-normal/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/2066/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Strange clog not normal.]]></description>
		<lastBuildDate>Fri, 19 Apr 2013 23:55:35 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20419/#p20419</link>
			<description><![CDATA[<p>You should take it all apart and find which part is plugged up and fix it by acetone, burning or drilling depending on which part.</p>]]></description>
			<author><![CDATA[null@example.com (pcpoirier)]]></author>
			<pubDate>Fri, 19 Apr 2013 23:55:35 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20419/#p20419</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20416/#p20416</link>
			<description><![CDATA[<p>So is there any solution for this problem? Also I would rather by a replacement part instead of the whole hotend, so what part should I buy?</p>]]></description>
			<author><![CDATA[null@example.com (Jonny)]]></author>
			<pubDate>Fri, 19 Apr 2013 23:40:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20416/#p20416</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20120/#p20120</link>
			<description><![CDATA[<p>Thanks Gordym, I might have to take you up on that. I have to set aside printing issues for a few weeks though till school settles down.</p>]]></description>
			<author><![CDATA[null@example.com (coleke)]]></author>
			<pubDate>Tue, 16 Apr 2013 15:06:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20120/#p20120</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20099/#p20099</link>
			<description><![CDATA[<div class="quotebox"><cite>coleke wrote:</cite><blockquote><p>Bought a pair of these on eBay: [url]2x HotEnd Fully Assembled and Wired +FREE Hobbed Bolt RepRap 3D Printer Hot End[1.75 mm,16 mm,other available sizes][/url]<br />Though, this &quot;looping&quot; problem occurred on these hotends as well. Compounding this problem is not having another printer to fix and tweak the extruder mounts to correctly hold the hotend.</p></blockquote></div><p>I live about 45 minutes south of Jackson (Adrian, MI). If you want a part printed, let me know and I can mail it to you.</p>]]></description>
			<author><![CDATA[null@example.com (Gordym)]]></author>
			<pubDate>Tue, 16 Apr 2013 13:02:24 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20099/#p20099</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20055/#p20055</link>
			<description><![CDATA[<p>Bought a pair of these on eBay: [url]2x HotEnd Fully Assembled and Wired +FREE Hobbed Bolt RepRap 3D Printer Hot End[1.75 mm,16 mm,other available sizes][/url]<br />Though, this &quot;looping&quot; problem occurred on these hotends as well. Compounding this problem is not having another printer to fix and tweak the extruder mounts to correctly hold the hotend.</p>]]></description>
			<author><![CDATA[null@example.com (coleke)]]></author>
			<pubDate>Mon, 15 Apr 2013 21:42:32 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20055/#p20055</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/20052/#p20052</link>
			<description><![CDATA[<p>Coleke, what have you been doing just buying a new barrel or PEEK or something else?</p>]]></description>
			<author><![CDATA[null@example.com (Jonny)]]></author>
			<pubDate>Mon, 15 Apr 2013 21:30:04 +0000</pubDate>
			<guid>https://www.soliforum.com/post/20052/#p20052</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19916/#p19916</link>
			<description><![CDATA[<p>Yeah that&#039;s exactly what it does. It extrudes maybe 15mm not sure than it bends. Also what is weird that I forgot to say is if the temperature is still on after the filament is out, slightly melted filament left in the barrel tends to creep out slowly from the top. Which I think that is from heat rising.</p>]]></description>
			<author><![CDATA[null@example.com (Jonny)]]></author>
			<pubDate>Sun, 14 Apr 2013 18:59:37 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19916/#p19916</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19897/#p19897</link>
			<description><![CDATA[<p>I have been having the same problem, with multiple hot ends. First was the hot end barrel and heater element from Qu-bd. Then my PEEK barrel broke when making sure it was snug against the barrel. Now I am having the same problems with a hot end I ordered on ebay. When you get it to extrude, does it start to print, then bend the plastic in loops between the peek and extruder motor?</p>]]></description>
			<author><![CDATA[null@example.com (coleke)]]></author>
			<pubDate>Sun, 14 Apr 2013 14:22:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19897/#p19897</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19820/#p19820</link>
			<description><![CDATA[<p>I got the new barrel from makergear with both ends turned down which I think is the same type as the solidoodle type. Also I did think that the PEEK wasn&#039;t tight enough at first so I cleaned out the barrel and nozzle and tightened but it&#039;s still clogged. If I haven&#039;t cleaned the barrel/nozzle and I take the filament out and put it in it doesn&#039;t extrude at all. But if I clean it it extrudes some but hardly any and takes a lot of force to do so. Also I don&#039;t think any thermal past is in there because the barrel and nozzle are both new and also with my old barrel and nozzle (stock) I never used thermal paste and it had the same type of clog so that&#039;s why I think it&#039;s the PEEK.</p>]]></description>
			<author><![CDATA[null@example.com (Jonny)]]></author>
			<pubDate>Sat, 13 Apr 2013 13:23:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19820/#p19820</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19798/#p19798</link>
			<description><![CDATA[<p>So, the new barrel you got.... was it from SD or is it the same(but slightly different) maybe non-beveled end version barrel?</p>]]></description>
			<author><![CDATA[null@example.com (ronsii)]]></author>
			<pubDate>Sat, 13 Apr 2013 06:09:38 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19798/#p19798</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19792/#p19792</link>
			<description><![CDATA[<p>I&#039;m betting you haven&#039;t threaded it tightly enough into the PEEK. If you take the filament all the way out, then feed it in again, does it extrude? For how long?</p>]]></description>
			<author><![CDATA[null@example.com (elmoret)]]></author>
			<pubDate>Sat, 13 Apr 2013 04:33:46 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19792/#p19792</guid>
		</item>
		<item>
			<title><![CDATA[Re: Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19791/#p19791</link>
			<description><![CDATA[<p>I read another post about defective thermal paste that caused a clog. I do not know where this paste is located or how to tell if it is faulty. Maybe someone else can help you determine if this is the problem.&nbsp; If this is the case Solidoodle should replace the parts at no cost other than time.</p>]]></description>
			<author><![CDATA[null@example.com (frozensoda)]]></author>
			<pubDate>Sat, 13 Apr 2013 04:15:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19791/#p19791</guid>
		</item>
		<item>
			<title><![CDATA[Strange clog not normal]]></title>
			<link>https://www.soliforum.com/post/19785/#p19785</link>
			<description><![CDATA[<p>So first I had a clog a week ago and accidentally bent the barrel from getting it off. So i bought a new barrel and a new nozzle because i wanted to experiment with a .25mm nozzle. But I installed them both and I haven&#039;t printed a single thing because it&#039;s clog. Also I know the nozzle and barrel are the right temperature because I bought a cheap food thermometer and the temperature was around 230. The only conclusion I can come up with is that the PEEK is clogging but when I take it apart there is filament inside the barrel so there might just be a lot of friction I don&#039;t know.</p>]]></description>
			<author><![CDATA[null@example.com (Jonny)]]></author>
			<pubDate>Sat, 13 Apr 2013 01:51:01 +0000</pubDate>
			<guid>https://www.soliforum.com/post/19785/#p19785</guid>
		</item>
	</channel>
</rss>