<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — First layer not sticking to subsequent layers]]></title>
		<link>https://www.soliforum.com/topic/1958/first-layer-not-sticking-to-subsequent-layers/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/1958/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in First layer not sticking to subsequent layers.]]></description>
		<lastBuildDate>Thu, 04 Apr 2013 20:32:15 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: First layer not sticking to subsequent layers]]></title>
			<link>https://www.soliforum.com/post/18622/#p18622</link>
			<description><![CDATA[<p>Is that where the screw head is on the bed? Maybe not heating up there</p>]]></description>
			<author><![CDATA[null@example.com (jjcuff1)]]></author>
			<pubDate>Thu, 04 Apr 2013 20:32:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/18622/#p18622</guid>
		</item>
		<item>
			<title><![CDATA[Re: First layer not sticking to subsequent layers]]></title>
			<link>https://www.soliforum.com/post/18601/#p18601</link>
			<description><![CDATA[<p>Not quiet - the exteriour is solid, but as I pulled the model off the kapton, the bottom layer was sagging (though no cracks appeared in the surface.&nbsp; So it&#039;s like this little button, like a blister on the skin might be.&nbsp; </p><p>Usually when I pull the print off, the bottom is hot, but very solid.</p>]]></description>
			<author><![CDATA[null@example.com (SpaceCowboy850)]]></author>
			<pubDate>Thu, 04 Apr 2013 17:39:33 +0000</pubDate>
			<guid>https://www.soliforum.com/post/18601/#p18601</guid>
		</item>
		<item>
			<title><![CDATA[Re: First layer not sticking to subsequent layers]]></title>
			<link>https://www.soliforum.com/post/18594/#p18594</link>
			<description><![CDATA[<p>Do you have the machine enclosed?&nbsp; Sometimes ambient air temp cools the layers too fast and they don&#039;t quite stick resulting in these &quot;gaps&quot; or &quot;air pockets&quot; as you call them.&nbsp; It looks like a horizontal crack in the wall of the part, doesn&#039;t it?</p>]]></description>
			<author><![CDATA[null@example.com (cckens)]]></author>
			<pubDate>Thu, 04 Apr 2013 16:58:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/18594/#p18594</guid>
		</item>
		<item>
			<title><![CDATA[First layer not sticking to subsequent layers]]></title>
			<link>https://www.soliforum.com/post/18590/#p18590</link>
			<description><![CDATA[<p>I have this post here:<br /><a href="http://www.soliforum.com/topic/1951/printing-advice-for-01mm/">http://www.soliforum.com/topic/1951/pri … -for-01mm/</a></p><p>And realized I might have posted in the wrong forum. </p><p>Has anyone ever experienced a print, where, the print sticks to the bed fine, but then, when you take the print off, there is an air pocket between the first few layers and the subsequent layers?&nbsp; I&#039;m not sure if it is just how Slicer sliced it or what.&nbsp; I&#039;ve never had this issue before.&nbsp; I&#039;m going to try to print a different object tonight and see if I see the same effect.</p>]]></description>
			<author><![CDATA[null@example.com (SpaceCowboy850)]]></author>
			<pubDate>Thu, 04 Apr 2013 16:45:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/18590/#p18590</guid>
		</item>