<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — SettingCoasting in Cura yes or no]]></title>
		<link>https://www.soliforum.com/topic/18662/settingcoasting-in-cura-yes-or-no/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/18662/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in SettingCoasting in Cura yes or no.]]></description>
		<lastBuildDate>Sat, 13 Jun 2020 14:48:12 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[SettingCoasting in Cura yes or no]]></title>
			<link>https://www.soliforum.com/post/153552/#p153552</link>
			<description><![CDATA[<p>I am printing with PETG Using CURA and still have a lot of problems with stringing do i need to turn on Coasting and if so<br />what settings.</p><p>Thanks<br />Dale</p>]]></description>