<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — need help with PETG settings]]></title>
		<link>https://www.soliforum.com/topic/18617/need-help-with-petg-settings/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/18617/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in need help with PETG settings.]]></description>
		<lastBuildDate>Sun, 01 Dec 2024 10:05:08 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: need help with PETG settings]]></title>
			<link>https://www.soliforum.com/post/157098/#p157098</link>
			<description><![CDATA[<p>it might be a little bit fast for <a href="https://kingroon.com/collections/petg-filament">PETG</a> since it&#039;s prone to stringing, and PETG is quite sticky, and if the retraction settings are not right, it can lead to oozing and blobs. You might try increasing the retraction speed and distance, such as setting the retraction speed to above 80mm/s and the retraction distance to 2mm.</p>]]></description>
			<author><![CDATA[null@example.com (Jimmyli)]]></author>
			<pubDate>Sun, 01 Dec 2024 10:05:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/157098/#p157098</guid>
		</item>
		<item>
			<title><![CDATA[Re: need help with PETG settings]]></title>
			<link>https://www.soliforum.com/post/153381/#p153381</link>
			<description><![CDATA[<p>Lower your nozzle temp and raise the bed temp to 80. Slowing down to 30 might help to. PETG will string and there is no way to prevent it. But you can limit it to just a little. Not like your print though.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Fri, 22 May 2020 20:51:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/153381/#p153381</guid>
		</item>
		<item>
			<title><![CDATA[need help with PETG settings]]></title>
			<link>https://www.soliforum.com/post/153376/#p153376</link>
			<description><![CDATA[<p>I want to use PETG for lithophanes but it is to Stringy I am printing at 35mm/s<br />what do i need to do. I am running Cura on an Ultimaker S3.</p><p>Thanks<br />Dale</p><p> <span class="postimg"><img src="http://soliforum.com/i/?InQXtkH.jpg" alt="http://soliforum.com/i/?InQXtkH.jpg" /></span><span class="postimg"><img src="http://soliforum.com/i/?sh0Kp6j.jpg" alt="http://soliforum.com/i/?sh0Kp6j.jpg" /></span><span class="postimg"><img src="http://soliforum.com/i/?QE65hHT.jpg" alt="http://soliforum.com/i/?QE65hHT.jpg" /></span></p>]]></description>