<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Help Filament 0m]]></title>
		<link>https://www.soliforum.com/topic/18239/help-filament-0m/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/18239/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Help Filament 0m.]]></description>
		<lastBuildDate>Tue, 08 Oct 2019 16:02:39 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Help Filament 0m]]></title>
			<link>https://www.soliforum.com/post/151618/#p151618</link>
			<description><![CDATA[<p>If it could be done, it would have by now. The printer is what remembers, not the software. There is no way around it.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Tue, 08 Oct 2019 16:02:39 +0000</pubDate>
			<guid>https://www.soliforum.com/post/151618/#p151618</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help Filament 0m]]></title>
			<link>https://www.soliforum.com/post/151617/#p151617</link>
			<description><![CDATA[<p>what if i install the printer again? rate a considerable number of nfca</p>]]></description>
			<author><![CDATA[null@example.com (danijelfurjan3)]]></author>
			<pubDate>Tue, 08 Oct 2019 15:47:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/151617/#p151617</guid>
		</item>
		<item>
			<title><![CDATA[Re: Help Filament 0m]]></title>
			<link>https://www.soliforum.com/post/151608/#p151608</link>
			<description><![CDATA[<p>The labels replace the RF chip on the spools. They can be set to 200m regardless of what the spool was as long as the original RF chip is removed from the spool. You can also just mount a new label on a blank spool to mount on the machine and just feed from another spool beside the machine. </p><p>Once a spool reaches zero the Rf chip cannot be reset. The machine remembers the serial number of each RF chip that reaches zero. Once it reaches 100 saved numbers it will push the first number out to make room for the next so you could reset the very first zeroed chip if you still had it after 100.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Tue, 08 Oct 2019 12:25:09 +0000</pubDate>
			<guid>https://www.soliforum.com/post/151608/#p151608</guid>
		</item>
		<item>
			<title><![CDATA[Help Filament 0m]]></title>
			<link>https://www.soliforum.com/post/151607/#p151607</link>
			<description><![CDATA[<p>Hello ..</p><p>My name is Daniel, I come from Croatia ..</p><p>I have a problem with the filament, so I got to 0m, and didn&#039;t know it needed to reset before it reached 0m, did it have any program to emulate the nfc chip ..</p><p>I tried via nfc key but it says it is locked, probably because I came to 0, I ordered the labels, and will those power be reset if I leave 1m of filament ..</p><p>This is an xyz mini maker</p><p>firmware 1.2.2.</p><p>chip <a href="https://imgur.com/a/CnVe4Lx">https://imgur.com/a/CnVe4Lx</a></p>]]></description>
			<author><![CDATA[null@example.com (danijelfurjan3)]]></author>
			<pubDate>Tue, 08 Oct 2019 11:29:12 +0000</pubDate>
			<guid>https://www.soliforum.com/post/151607/#p151607</guid>
		</item>
	</channel>