<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — new person looking for info from long term filastruder users]]></title>
		<link>https://www.soliforum.com/topic/17302/new-person-looking-for-info-from-long-term-filastruder-users/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/17302/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in new person looking for info from long term filastruder users.]]></description>
		<lastBuildDate>Sun, 06 May 2018 02:02:05 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: new person looking for info from long term filastruder users]]></title>
			<link>https://www.soliforum.com/post/143931/#p143931</link>
			<description><![CDATA[<p><span class="postimg"><img src="http://soliforum.com/i/?D8otdq9.jpg" alt="http://soliforum.com/i/?D8otdq9.jpg" /></span><span class="postimg"><img src="http://soliforum.com/i/?RCF0Wgj.jpg" alt="http://soliforum.com/i/?RCF0Wgj.jpg" /></span><br />My favorite thing about the filastruder is multi color parts that&#039;s gradually change colors</p>]]></description>
			<author><![CDATA[null@example.com (Kronikabuse)]]></author>
			<pubDate>Sun, 06 May 2018 02:02:05 +0000</pubDate>
			<guid>https://www.soliforum.com/post/143931/#p143931</guid>
		</item>
		<item>
			<title><![CDATA[Re: new person looking for info from long term filastruder users]]></title>
			<link>https://www.soliforum.com/post/143904/#p143904</link>
			<description><![CDATA[<p>It also depends on available shop space and the need aka how much filament do you use. I have had a printer for about 4 years and have actually emptied about 4 filament rolls and do not have a lot of space so no filasruder for me.</p>]]></description>
			<author><![CDATA[null@example.com (Tin Falcon)]]></author>
			<pubDate>Sat, 05 May 2018 15:51:48 +0000</pubDate>
			<guid>https://www.soliforum.com/post/143904/#p143904</guid>
		</item>
		<item>
			<title><![CDATA[Re: new person looking for info from long term filastruder users]]></title>
			<link>https://www.soliforum.com/post/143902/#p143902</link>
			<description><![CDATA[<p>I agree with Kronikabuse - you do save some on lower end stuff, but the real benefit to Filastruder is saving on the more exotic materials and/or using better quality raw materials.&nbsp; Eg - that $9-15 per KG PLA filament you mention is almost certainly NOT using Natureworks 3D850 or 3D870, yet for $11 you can buy 1KG of 3D870 pellets.&nbsp; Or another example - say you suddenly decide you want to see what happens when you make wood filled PETG (instead of the traditional wood filled PLA) - you can (just make sure you don&#039;t have the filter in on Filastruder and use a larger nozzle on printer).&nbsp; Wonder what happens when you mix in two different colors?&nbsp; You can.</p><p>Recently I saw some filament called &#039;marble&#039; filament - it&#039;s mostly white with black specks.&nbsp; I threw some extra fine glitter in and made sure that it would print fine still.&nbsp; Now I just need to get some black colorant, throw that white glitter in, and see what the opposite looks like (I&#039;m hoping less marble, and more granite).</p>]]></description>
			<author><![CDATA[null@example.com (genesat1)]]></author>
			<pubDate>Sat, 05 May 2018 15:43:31 +0000</pubDate>
			<guid>https://www.soliforum.com/post/143902/#p143902</guid>
		</item>
		<item>
			<title><![CDATA[Re: new person looking for info from long term filastruder users]]></title>
			<link>https://www.soliforum.com/post/143888/#p143888</link>
			<description><![CDATA[<p>Recycling old plastic is nice but you always have to add virgin material. All plastic has a life span where it becomes unusable. Im not sure about the break even point. But like reloading ammo, you don&#039;t really save on .223 or standard material types. You&#039;ll save on the not so common uses .You&#039;ll also get a higher quality product. More choices like colors. I have a filastruder and filwinder. It&#039;s a nice addition to the shop</p>]]></description>
			<author><![CDATA[null@example.com (Kronikabuse)]]></author>
			<pubDate>Fri, 04 May 2018 18:23:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/143888/#p143888</guid>
		</item>
		<item>
			<title><![CDATA[new person looking for info from long term filastruder users]]></title>
			<link>https://www.soliforum.com/post/143887/#p143887</link>
			<description><![CDATA[<p>just wondering what the breakeven point is for extruding your own PLA for printing, with prices of filament wandering around $15-$9/k</p><p>I see sources of pla between 5-8/k so that would be a breakeven of 50-60 kilos?</p><p>I&#039;d like to pull the trigger on a filastruder unit, to help recycle plastic and reuse all my empty spools, since it looks like masterspool isn&#039;t taking off</p>]]></description>
			<author><![CDATA[null@example.com (tater1337)]]></author>
			<pubDate>Fri, 04 May 2018 17:45:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/143887/#p143887</guid>
		</item>